Electronics Forum | Tue Mar 01 15:07:00 EST 2011 | dennisfo
Update on 1B73 bubbles, Changed over to a mixture of Humiseal 73 thinner with coating (25 sec on Zahn 2) observed a reduction in bubble formation (approx. 20%) but still present.
Electronics Forum | Thu Dec 15 10:43:51 EST 2005 | chunks
Hi Amol, We use the PVA system and also conformal coat over no-clean reflow solder as well as no-clean wave. We use a Humiseal coating and thinner.
Industry News | 2013-03-23 04:16:57.0
Drive Technologies offer a large stock of popular HumiSeal coating materials such as 1B31,1B73LED,1R32A2,Thinner 521 at attractive prices.No MOQ restrictions.
Industry News | 2008-08-07 16:15:33.0
DENVER � August 2008 � Krayden, Inc., a leading distributor of engineered materials, announces that it will exhibit technologies from its industry-leading suppliers in booth 330 at the upcoming SMTA International exhibition and conference, scheduled to take place August 19-20, 2008 in Orlando, FL.