Electronics Forum | Wed Oct 22 12:13:18 EDT 2008 | brismittr
A no-clean paste with an above average amount of halides should do the trick. Kester EP256HA is a good choice for this application if you are using a leaded alloy (Sn63 or Sn62).
Electronics Forum | Tue Jul 06 10:46:12 EDT 2004 | blnorman
We have now switched to Kester EP256. During our solder paste evaluation, resistance to humidity was one of the selection criteria. We printed multiple boards, then exposed them to 85�F/65% RH. At 30 minutes, 1 hour, 2 hours, and 4 hours exposure