Electronics Forum | Sun Jan 30 21:56:05 EST 2000 | Paulvannan
We used Promosol Sn96.5/Ag 3.5 during our initial qualification for similar application. We could not achieve a shiny solder joint. Our changes to Sn95.5/Ag 4.5 does not improve the look. In order to confirm the reliability of the joint, I suggest yo
Electronics Forum | Wed Mar 21 11:42:54 EDT 2012 | davef
Downhole solder suggestions, in order of preference are: * Kester Sn96.3Ag3.7. Most vendors do not stock straight tin-silver alloys, whose wallet is that fat? * SAC305 can usually be used in place of one of the copper-free tin-silver alloys in downho
SMT Express, Issue No. 3 - from SMTnet.com Volume 1, Issue No. 3 Wednesday, August 18, 1999 Featured Article Return to Previous Page BGA REWORK Earl Moon Proof Of Design (POD) SOLDER PASTE APPLICATION (WHEN AND AS SPECIFIED) Select