Electronics Forum: 1b31 bubbles after ess (Page 1 of 1)

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Fri Dec 18 09:07:24 EST 2009 | tommyg_fla

dave, where I work they are having the same problems with 1B31 acrylic. The coating thickness is 6-8 mils dried so that have to do several passes with an air dry between them and a final oven cure. They think that it might be related to the heating r

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Mon Dec 28 09:12:56 EST 2009 | kpm135

@tommyg_fla According to the TDS the recommended coating thickness for Humiseal 1B31 is only 1-3 mils so if I had to guess I would say your issue might be that you're re-coating over the first pass too soon. All the solvent hasn't evaporated and the

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Fri Dec 18 09:27:51 EST 2009 | sforman1

Tom: Once again - why are you using solvent based conformal coating. 1B31 is OK as a CC but it contains Toluene and MEK!! It is only 35% solids which means you are trying to get rid of 65% solvent. If you must use it due to customers requirement then