Electronics Forum | Mon Sep 06 23:23:24 EDT 2004 | laxman
recently we bought Cyber Optic's LSM2 Solder paste height measuring system and we want to conduct SPC.Can anybody guide in this regard?
Electronics Forum | Mon Sep 25 07:49:31 EDT 2006 | egrice1@wi.rr.com
Check out ERSA's Ecoselect 350. You can have 2 solder pots in the machine. 1 for SN/PB and 1 for Lead Free. It's a little more than $ than the others, but its a production machine! Not a toy.
Electronics Forum | Tue Sep 09 13:03:19 EDT 2008 | logannsan
What is this? I thought 63sn 37pb was the norm. What is with the 2 at the end? Anyone know?
Electronics Forum | Tue Sep 09 16:39:03 EDT 2008 | vladig
As far as I know, they rarely do it with Pb-bassed solders. Pb-free may contain Cu or Ni (to improve test performance) Vlad
Electronics Forum | Wed Sep 10 16:53:46 EDT 2008 | realchunks
Actually it's not rare. I use several pastes from various manufacturers that add 2% silver in their leaded pastes. I would bet it's 2% silver.
Electronics Forum | Wed Sep 10 17:08:08 EDT 2008 | slthomas
Isn't that the non-eutectic one that provides the pasty phase range that people use to clobber their tombstoning problems?
Electronics Forum | Thu Sep 11 02:54:27 EDT 2008 | cobar
The 2 % is Ag.It is added to prevent leaching silver from the end caps of components.This alloy like 63/37 is eutectic and has a reflow temp of 179�C whereas 63/37 is 183�C.
Electronics Forum | Mon Jul 15 11:36:18 EDT 2013 | rgduval
Some great legal language here, Dave. Guess some people don't like their knowledge being shared. Probably shouldn't publish it to the interwebs if that's the case.
Electronics Forum | Tue Oct 08 10:16:39 EDT 2019 | leeg
We used a similar part and adjusted the routing so that the front edge of the connector was supported and therefore keeping the connector flat and it not being able to tip forward. I don't know if this is something that you can do with your board?
Electronics Forum | Fri Nov 13 03:57:41 EST 1998 | Steve Cheung
We are experiencing 'lifting' on one or more sides of a QFP. Poor lead co-planarity has been ruled out by independent tests. Please tell me which of the two remaining failure modes is the most probrable? 1. Expansion of gases in vias underneath devi