Electronics Forum | Wed Aug 21 17:50:05 EDT 2002 | davef

First, it�s GREAT that your defect rate of 282 is very close to your Boss� goal of 50 ppm. Second, your Cpk and your ppm numbers don�t tie out with our expectations. You say Cpk for: * mounter is 1.0 and �your mounting is 83ppm�. * printing is 1.33

Why 50 mils in 0805 package instead of 40 mils.

Electronics Forum | Fri Oct 03 09:00:18 EDT 2003 | davef

EIA standard packages have a variety of L/W proportions. EIA||Dimension mm (LXW)||Proportion (L/W) 0201||0.6X0.3||2 0202||0.5X0.5||1 0303||0.8X0.8||1 0402||1.0X0.5||2 0504||1.25X1.0||1.25 ||1.4X1.4||1 0603||1.6X0.8||2 0805||2.0X1.25||1.6 1111||2.8X2

Stencil Manufacturer

Electronics Forum | Mon Mar 13 10:03:34 EDT 2017 | oxygensmd

Depends on where are you located? If you are from EU, I can recommend a 4-5 manufacturer.

Baking Moisture Sensitive Components >4.5mm

Electronics Forum | Mon Jan 22 14:22:46 EST 2007 | muse95

Actually, I've been looking into this myself, and the B version doesn't help any more than the A version. The tables still only go to 4.5mm. And Appendix B has a bunch of formulas with undefined variables that I haven't been able to figure out. An

GSM Placement Offset

Electronics Forum | Wed Jun 17 17:53:48 EDT 2020 | aveazey

We've got a GSM1 running OS2/WARP version 4.5.0 and we ran into having placement issues for all components. Each placement seems to be exactly 30 mils offset from it's actual location. We've got a 2.6 mil/px and a 4.0 mil/px camera. Attached is an

Shoot Up Reflow Zone

Electronics Forum | Mon Jan 30 22:45:30 EST 2017 | cmarasigan

Hello Marc, Thank you for the recommendation. I've contacted our local service support. We found out that heat coming from higher zones 7, 8 & 9 overflows to zone 3, 4 & 5 which affects actual temp reading at Z3,4,5. Since we already replaced some b

Stencil thickness

Electronics Forum | Thu Jun 16 18:19:05 EDT 2005 | Jason Fullerton

If the uBGA has aperatures that are 0.25mm square, you need to use a laser cut foil no thicker than 3.75 mils to get an area ratio of 0.67, which is the minimum rule of thumb - that's too thin! Electroform would probably work up to 4.5 mils thick.

28 pin QFN Pads.

Electronics Forum | Thu Sep 16 17:56:48 EDT 2010 | asksmt

Ok Thanks, i have reduced thermal pad size by 4.5 mils on top and bottom part of this footprint where the problem was occuring, so now the clearance between thermal pad and lead pads are 12 mils instead of 7.5 mils on two sides. (i kept the signal pa

Looking For Platform Set-up Validation (PSV) for UPS 4.5e (OS/2) Software

Electronics Forum | Fri Apr 17 12:09:21 EDT 2015 | ilavu

Hello All, I am in need for "Platform Set-up Validation" (PSV) for my Universal GSM2 with UPS version 4.5. My installation disk for PSV is bad and can not reinstall after hard drive crash.My machine is not register with Universal because some serial

  1 2 3 4 5 6 7 8 9 10 Next

4-5 0 searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

High Precision Fluid Dispensers
Best SMT Reflow Oven

High Throughput Reflow Oven
Fluid Dispensing, Staking, TIM, Solder Paste

Reflow Soldering 101 Training Course


Best Reflow Oven


SMT & PCB Equipment - MPM, DEK, Heller, Europlacer and more...