Electronics Forum: 94v (Page 1 of 2)

Intrusive reflow component selection

Electronics Forum | Mon Jul 10 04:16:03 EDT 2006 | dougs

Hi, We have a new product coming soon that has a fair number of PTH sockets and headers. I was thinking that it would be good to use intrusive reflow on some of them to even up cycle times between SMT and hand insertion, however, when i called t

Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 12 19:28:26 EDT 1999 | Tom B

Netters, When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? 1. Kester 293 no clean 2. 2.1 C/s for 30s to 150 C 3. .5 - .7 C/s for 60s to 185 C 4. 1.5 C/s u

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 18:11:00 EDT 1999 | Jimmy Strain

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 11:21:03 EDT 1999 | Travson

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 20:49:13 EDT 1999 | Dave F

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Printed Circuit Board Material

Electronics Forum | Wed Oct 18 16:41:35 EDT 2000 | Dave F

It's unrealistic to think that two materials with the following disperant properties would have the same reflow profile. From http://www.norplex.com/Carrier.htm Physical Properties / NEMA FR-4 / NEMA CEM-1 Glass transition temperature �C / 130 / 10

What is needed for UL ?

Electronics Forum | Tue Sep 12 12:43:26 EDT 2017 | deanm

50) traces. The design will be tested for safety and a file will be created listing all the critical components such as transformers, relays, wiring, enclosure material, etc. On the manufacturing side, a manufacturing facility must be indicated in

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 18:39:24 EDT 1999 | Tom B

| | Netters, | | | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | | | 1. Kester 293 no clean | | 2. 2.1 C/s for 30s to 150 C | | 3. .5 - .7 C/s f

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 23:08:56 EDT 1999 | Jeff Sanchez

| | | Netters, | | | | | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | | | | | 1. Kester 293 no clean | | | 2. 2.1 C/s for 30s to 150 C | | | 3.

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Wed Apr 21 00:35:31 EDT 1999 | Scott Cook

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185