Electronics Forum | Tue Jun 07 12:07:30 EDT 2016 | wlsmt
Sorry davef. I was not being clear. PCBAs came out cold soldered after being reflowed the first time with ALPHA WS-820. The flux gel ALPHA WS 609 was supposed to be applied only onto the terminations of caps where ALPHA WS-820 was for a second refl
Electronics Forum | Wed Jun 15 10:38:41 EDT 2016 | laynefelix
Hi everyone..i am new here. I am hardware design engineer and as per my experience PCBAs came out cold soldered after being reflowed the first time with ALPHA WS-820. The flux gel ALPHA WS 609 was supposed to be applied only onto the terminations of
Electronics Forum | Mon Jun 06 12:51:17 EDT 2016 | wlsmt
My operator applied flux gel ALPHA WS-609 on MG P/N FTH101XAP (CAP ALUM 100UF 50V 20% SMD) before aqueous washing the PCBAs. Solder paste used was ALPHA WS-820. Now the caps have yellow stains. Any solution to this is appreciated. Tks
Electronics Forum | Tue Jun 07 10:24:59 EDT 2016 | davef
wlsmt: You’ve got to help us out here: * Why did you apply solder paste to capacitors prior to water washing the PCBA [where the caps were attached?]? * Did you reflow the Alpha WS-609? * How is the Alpha WS-820 involved in this? * Talk about the
Electronics Forum | Thu Aug 15 17:05:54 EDT 2013 | srgbarba
Hi, I'm using WS-820 by Alpha metals and works good, but you must take in consideration the humidity and temperature that you have in your facility, In the process that we're following we left the board printed during 2 hrs and works ok (no pop up ef
Electronics Forum | Fri Jan 24 09:52:08 EST 2014 | davem
Hi Guys, So I work for a small contract manufacturer which caters mainly to the defense sector. As such, our customers haven't (yet) had a great need to incorporate 01005's into their designs. Looking forward, we decided to "take the plunge" and dia