Hi, we have an used ASSCON VP450. But tghe time in - out of the PCB is about 25 minutes. Very high time. The most long time is in pre-heating fase. EDR=100% Have you any ideas to configure it? Thank you

Manufacturers of

Electronics Forum | Fri Nov 19 13:46:14 EST 2004 | Dreamsniper

I used ASSCON VP450 with Galden 205 Fluid. It worked fine. Good Solder Joint Quality. I'm not promoting the product just sharing what I had.

ASSCON VP450

Electronics Forum | Tue Jul 30 06:43:57 EDT 2024 | mirkospada

Thank you for the answer. The problem is that all the cycle is between 15 and 20 minutes. We have checked the heat resistor and it is ok.

ASSCON VP450

Electronics Forum | Mon Jul 29 20:41:24 EDT 2024 | bsziszi

It is normal to have a longer heat up time when you power on the machine. Then the cycle time depends on your board mass and oven settings. (We have a bigger Ascon oven and the cycle time after the initial heat up is between 5-10 min @ 50% ETR). If y

ASSCON VP450

Electronics Forum | Tue Jul 30 14:17:38 EDT 2024 | bsziszi

Maybe check your sensors and the parameters for soldering. Do you see any promp during soldering that the solder cycle exceedes the maximum soldering time? Are you using ASB? Have you measured the soldering profile? (Does it confirm the long solderin

  1  

asscon vp450 searches for Companies, Equipment, Machines, Suppliers & Information

used smt parts china

High Resolution Fast Speed Industrial Cameras.
High Throughput Reflow Oven

Reflow Soldering 101 Training Course
Win Source Online Electronic parts

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
SMTAI 2024 - SMTA International

Best Reflow Oven