ATF selective soldering machine(s)

Electronics Forum | Wed Oct 13 15:45:04 EDT 2021 | dilogic

Does anybody have experience with ATF's selective soldering machines? Information on the web is scarce and their responses to my queries are either none or very limited. Any information is welcome...

selective soldering approch

Electronics Forum | Sun May 09 22:56:14 EDT 2004 | snehal acharya

hi everybody, can anybody give the manufacturer's name of good selective solder M/C. Snehal Acharya.

selective soldering approch

Electronics Forum | Mon May 17 08:44:58 EDT 2004 | solderpro

Vitronics or Ursa

Entry level selective soldering

Electronics Forum | dwl |

Tue Jul 06 17:41:14 EDT 2021

selective soldering approch

Electronics Forum | Fri May 21 11:20:42 EDT 2004 | Cal

We actually use a solective soldering fixture for our wave soldering process. cal

selective soldering machines

Electronics Forum | Wed Jun 02 09:10:30 EDT 2004 | dougm

My company is looking at the various options for selective soldering machines. We are mostly a low volume, high mix facility, with some moderate volume orders as well. I have looked at the Pillarhouse Topaz XL, Ersa Versaflow, and Vitronics Soltec

selective soldering approch

Electronics Forum | Mon May 10 22:49:45 EDT 2004 | snehal acharya

Hi to ALL, pls give the details about Selective solder M/C Manufacturer.(site detials),if any one knows. regards, Snehal

lead free selective soldering

Electronics Forum | Wed Nov 02 12:08:40 EST 2005 | chunks

It could be lack of preheat or flux. You can verify the flux by hand applying. I'll bet it's lack of preheat though. That's usually the case with selective solder.

ZSWHPS-12S selective soldering machine

Electronics Forum | Mon Aug 02 17:09:12 EDT 2021 | alexeyzb

What do you think about ZSWHPS-12S selective soldering machine? It looks like Ersa but more cheaper. Please, can you give me some advantages and disadvantages? I need facts, which i can check.

lead free selective soldering

Electronics Forum | Thu Nov 03 09:43:55 EST 2005 | lupo

Check flux penetration and type of flux. How much is solid contents. The solder filling is better under Nitrogen. Check the time (speed) of the nozzle whether is correct. Usually For SAC305 the temperature of bath is 320C/degrees, but only for sel

  1 2 3 4 5 6 7 8 9 10 Next

atf selective soldering searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Best Reflow Oven
pressure curing ovens

We offer SMT Nozzles, feeders and spare parts globally. Find out more
Global manufacturing solutions provider

High Precision Fluid Dispensers