Electronics Forum | Wed Nov 29 00:43:45 EST 2006 | callckq
Dear all, Recently, we run 2 models with heat sink attachment on top of this BGA(on top of this BGA, there is flip chip attached at the center of the BGA). Hence, the center of the BGA is higher than corner/side. We used conventional way to attach
Electronics Forum | Mon May 10 16:37:01 EDT 2004 | davef
First some definitions, the two main types for solder masking near BGA pads are: 1 Pad, Non-Solder Mask Defined. In circuit board design, pads with spacing that does not allow solder (usually bumps) on the pads to contact the adjacent solder mask. [
Electronics Forum | Thu Dec 07 14:23:30 EST 2006 | russ
I wuld say it is attachment method and post install force that is the problem not the size of the heatsink. we place heatsinks that are at least 5 times the size of BGA with no issue, they are attached with very precision torque drivers. Russ
Electronics Forum | Thu Dec 07 10:10:49 EST 2006 | Learn from U
Hello, I need your advice..Welcome any input!! Cheers..
Electronics Forum | Fri Feb 19 05:14:04 EST 2016 | truewanderer
Hi, i have a confusion to read the dimension of BGA package from the datasheet. I have attached the datasheet below. Is this diameter of the ball 0.30mm or 0.15mm. I'm confused about the values given in the box. Whats meant by M, S, A and B. Please g
Electronics Forum | Thu Feb 21 13:08:06 EST 2002 | vincent_f
Hello, I had recently a problem of crack between the solder ball (SnPb) and the Ni layer of the PCB pad. We use Electroless Ni/Au technology for PCB. This phenomena is amazing because the crack is very clean (straight) and it creates a space betwee
Electronics Forum | Thu Sep 12 10:45:29 EDT 2002 | pbarton
We have used a laser cut stencil 0.15mm (0.006") thick with 0.3mm (0.012") square apertures radiused in the corners 0.06mm (0.0025") to aid paste release. This approach with the (type 3) paste we use has proven successful on thousands of devices plac
Electronics Forum | Fri Feb 01 14:23:47 EST 2002 | delnosa
Looking for help on getting information on understanding the physics of micro-fracture growth rate within the BGA ball (or solder joints in general). Hoping to find a fairly straight forward study on the concept/theory of this topic. I'm not a meta
Electronics Forum | Thu Sep 24 09:25:24 EDT 2009 | davef
What do you mean by "substrate?" Is it: * Semiconductor die * BT circuit board interposer Is the BGA package: * Encapsulated * Mounted on a circuit board
Electronics Forum | Mon May 25 08:37:28 EDT 2009 | d0min0
Hello, recently we changed supplier of the LF BGA, we did corossection and now have doubts... previous BGA specs : pitch 1mm, ball diameter 0.6mm future BGA specs : pitch 1mm, ball diameter 0.4mm on the crossecrion we found that one of the ball seem