Electronics Forum | Mon Jan 29 11:14:44 EST 2001 | medernach
Hi all, Here's the deal. I have a customer for whom I assemble a lot of product. All of their product mix goes through a water soluble process. Much of it gets conformal coated. They are in the high power arena but some products are simply contro
Electronics Forum | Sat Jan 06 22:09:53 EST 2001 | Greenman
Cory, I've got a lot of experience of testing of this type. The physical (not chemical) nature of the flux residues is the crucial issue in compatibility. If you have a softer residue (either caused by a thick initial solder paste deposit, or a low p