Electronics Forum | Wed Mar 04 10:23:03 EST 2015 | rgduval
I haven't used this particular CC, but...found this in their data sheet: "AVR 80 BA Conformal Coating will be touch dry after 15 - 20 minutes at room temperature and does not require a thermal cure. The full properties of the coating will be obtaine
Electronics Forum | Wed Mar 04 10:59:24 EST 2015 | jpierre
Hi first DS65 version is a specific dilution for dispensing machine, in this case the typical process is following: application of the conformal coating extraction of solvent (low extraction power is better)2minutes and drying the drying can be done
Electronics Forum | Wed Jan 27 09:00:56 EST 1999 | Chris Fontaine
| | I have boards coated with Humiseal 1B73. At a late point mfg. site we need to remove a series of 0603 resistors for optioning purposes. I have been trying to determine the fastest, easiest way to re-coat the pads after removal. Drying time of the
Electronics Forum | Sun Nov 22 19:53:10 EST 2009 | prodrivegsr
Hi Ju Yong, The PCB are dry in an airseal cabinet(Staging Chamber) before IR Oven. The bubbles show at around body and solder joint area. You mean the moisture will create bubbles ? Able to advice the humidity and temperature that you are using in
Electronics Forum | Tue Nov 24 05:23:18 EST 2009 | prodivegsr
Hi Davef, Thanks...Saw 1 of your thread that you posted : Thanks for providing... From davef : There are many possibilities: * Conformal coat is incompatible with surface residue on the board * Conformal coat is incompatible with solder mask on the
Electronics Forum | Thu Aug 27 11:35:07 EDT 2009 | davef
There are many possibilities: * Conformal coat is incompatible with surface residue on the board * Conformal coat is incompatible with solder mask on the board * Moisture is out-gassing from the board * Conformal coat is too thick and does not allow
Electronics Forum | Wed Mar 11 16:43:20 EDT 2020 | sumote
There is a 8lb steel plate that is held down by 4 toggle bolts at the top of the machine. Its where you load the cutting media. If that plate does not have a pressure gauge built into it, contact CCR. They will send you one free of charge (at least t
Electronics Forum | Wed Jun 29 14:36:11 EDT 2005 | Steve
A customer of mine is using Chemtronics (Circuit Works) CW3300 Overcoat pen. This is an acrylic conformal coating. It cures at Room temperature. They need something similar that can be UV cured in a pen form. Any suggestions?
Electronics Forum | Sat Apr 21 12:06:43 EDT 2007 | Cmiller
I coated three other bare boards on one side this morning from two different suppliers. Two of them had exceptional adhesion and one was so-so. I ran them through the reflow oven, coated them and got the same results on the other side, so it does not
Electronics Forum | Sat Jan 06 22:09:53 EST 2001 | Greenman
Cory, I've got a lot of experience of testing of this type. The physical (not chemical) nature of the flux residues is the crucial issue in compatibility. If you have a softer residue (either caused by a thick initial solder paste deposit, or a low p