Electronics Forum | Tue Apr 13 11:41:18 EDT 2021 | jeremy_leaf
I have a SAC305 preform with which I am attempting to bond a gold coated component to an ENIG coated PCB pad. I've specified 2 microinches of gold for the ENIG. It worked previously but now with a new batch of boards, I am having an issue where the p
Electronics Forum | Fri Nov 08 17:49:05 EST 2013 | davef
First, it's a surprise that your failure analysis lab thought everything was OK with these boards. They look like shit. Second, a few years ago, there was a bunch of complaints about ENIG boards with issues similar to what you're observing. There wa
Electronics Forum | Fri Apr 29 14:16:16 EDT 2011 | ppcbs
Below is the long explanation. This defect is most commonly found with BGA components, but can arrise with all components. I see it happening more now with lead free boards that are being assembled with a no clean flux. Best short term remedy is t
Electronics Forum | Wed Oct 24 18:08:02 EDT 2001 | davef
1- DF1: WOW!!! How do people get these cool toys? CB: I am with the University at Buffalo Electronic Packaging Lab. http://www.packaging.buffalo.edu We have pretty much everything that is sold on the market as well as Laser inspection technologies we