Dave, We are using Kester Easy Profile 256 No clean Sn62Pb36Ag02. The oven itself is a Dima SMRO-0252 which is a short oven, it has 13" of preheat, 13.5" of soak, 6.25" of reflow, and 10" of cooling on the way out of the oven. We are soldering multi
Electronics Forum | Mon Nov 29 01:58:43 EST 2010 | leo_dektec
Hello Sir, Here is a link you can take look. http://www.deksmt.com The machine I would like to recommend you is BM-W430 and BM-W630. We are a major manufacture of reflow oven and wave solder in China, till now we have distributos in more than 16
Electronics Forum | Mon Jul 27 13:59:11 EDT 1998 | Robert Steltman
We are about to run our first BGA devices and would appreciate some confirmation on a few points. First some details: PCB & Device: ============= 1) 16 layer (4 power, 4 gnd, 8 signal) 2) gold on nickel finish 3) ceramic BGA with eutectic balls Refl
Electronics Forum | Tue Jul 28 02:13:57 EDT 1998 | Bob Willis
There is a procedure for profiling on my web site that may be of use to start with www.bobwillis.co.uk | We are about to run our first BGA devices and would appreciate some confirmation on a few points. | First some details: | PCB & Device: | ======
Electronics Forum | Tue Jul 28 02:22:59 EDT 1998 | Bob Willis
Here is what I would do faced with your problem. First I would profile a similar board or use an existing profile. From there I would place the dummy device on the surface of a sample board with a thin thermocouple soldered to the board surface under
Electronics Forum | Tue Jul 28 09:15:49 EDT 1998 | Justin Medernach
| We are about to run our first BGA devices and would appreciate some confirmation on a few points. | First some details: | PCB & Device: | ============= | 1) 16 layer (4 power, 4 gnd, 8 signal) | 2) gold on nickel finish | 3) ceramic BGA with eutec
Electronics Forum | Tue Jul 28 17:23:58 EDT 1998 | Robert Steltman
| | We are about to run our first BGA devices and would appreciate some confirmation on a few points. | | First some details: | | PCB & Device: | | ============= | | 1) 16 layer (4 power, 4 gnd, 8 signal) | | 2) gold on nickel finish | | 3) ceramic
Electronics Forum | Wed Dec 10 16:58:53 EST 2014 | sreejhu
Hello, yes you are absolutely correct. I agree with your point. Last week,I personally checked out my board on Heller 1088 which is a 8 zone reflow oven (4 on top and 4 on bottom) and the soldering came pretty nice. So comparing with that situation
Electronics Forum | Thu Dec 11 09:15:06 EST 2014 | sreejhu
Hello Sir, Thanks for your reply. i just got a mail from the DIMA service group and they said the Oven setting is as follows: Max temp settings in each zone (Which is not the temperature on your product, but close to where the air flow comes out of
Electronics Forum | Thu Dec 11 08:22:26 EST 2014 | emeto
The longer the oven, the better. You will have much more capabilities in creating the precise profiles the way you want them(with10-12 zone oven). I have worked with ovens from 2 to 12 zones and the difference is huge. In my opinion try to get a 10zo