Electronics Forum | Thu Apr 22 10:57:20 EDT 1999 | Jack Coia
On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although when ot
Electronics Forum | Mon Oct 24 17:56:57 EDT 2005 | Ali
Hello all: A couple of queries on matte Sn plating: My Application: 2 Reflows in subassembly reflow+ 8 Hr Steam age+ Solderability (Dip and look) for sub assembly to mother board soldering. Queries on Matte Sn: 1- Different plating vendor
Electronics Forum | Thu Apr 22 13:20:04 EDT 1999 | Ben Kirk
| On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although when
Electronics Forum | Thu Apr 22 14:36:33 EDT 1999 | Dave F
| On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although when
Electronics Forum | Thu Apr 22 18:07:38 EDT 1999 | Tom B.
| On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although when
Electronics Forum | Thu Apr 22 20:26:39 EDT 1999 | Dave F
| | On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although whe
Electronics Forum | Thu May 01 18:37:31 EDT 2003 | gregoryyork
Did you get any dulling of the solder joints at all or importantly was the resist discoloured or bleached after cleaning. It is possible to absorb flux and saponifier into the resist and this will definately cause poor SIR or electromigration especia
Electronics Forum | Mon Jan 21 11:41:39 EST 2019 | SMTA-Tony
Lead free HASL coatings can be susceptible to yellowing during reflow due to oxidation of the tin in the coating. Some HASL solder suppliers use anti-oxidant additives in the solder to limit or prevent yellowing of the coating. You may want to ask
Electronics Forum | Sun Jan 25 17:40:16 EST 2009 | cuperpeter
Hello All, I have a problem with nonwetting Au finish after second cycle of reflow soldering doublesided boards. Solder nonwetted pcb pads (is wicked to component terminations) Either these pads or some of non component pads became discoloured from
Electronics Forum | Tue Feb 03 16:42:50 EST 2009 | cuperpeter
Hello All, > > I have a problem with nonwetting Au > finish after second cycle of reflow soldering > doublesided boards. Solder nonwetted pcb pads (is > wicked to component terminations) Either these > pads or some of non component pads became