Electronics Forum | Fri Nov 07 15:57:56 EST 2003 | Marc Simmel
Are there specifications or recommendations for electro-deposited tin-lead plating thickness on austenitic stainless steel that would provide a shelf life of 1 year? 6 months? Would 2 to 3 microns (78 to 118 micro-inches) 90/10 tin-lead over 1.27 mi
Electronics Forum | Thu Dec 08 01:05:34 EST 2005 | Mike_Kennedy
Our new PCB supplier can give us a 20% price reduction if we convert from an ENIG finish to a FLASH gold finish. My uderstanding between the two is as follows: ENIG - Nickel is plated over copper and then immersed in Gold which forms a self limited f
Electronics Forum | Fri Dec 09 02:20:47 EST 2005 | Mike_Kennedy
Grant, I dont quite understand the implications my self yet on gold deposit using FLASH or ENIG. However the important part of the gold finish is that it is kept under 3% of the total solder joint, so normally its safe. With the FLASH process it is m
1 |