Electronics Forum | Wed Oct 04 14:46:46 EDT 2000 | Kal. Chak.
Hi folks, What are the differences between Epoxy resin(ER)conformal coating and adhesive stacking/bonding material? My PSA/PRA (Post solder/reflow assembly)bracket assembly process got some ER adhesive encroachment on pads/solderjoints. I have chec
Electronics Forum | Tue Feb 08 16:09:09 EST 2000 | dean
Generally speaking with most electronic grade epoxies: 1. Cure time is a function of temperature. 2. Polymer bonds begin to quickly break down above certain temperatures (product specific). I believe aprox 170-180C. The strength of the bond de
Electronics Forum | Mon Aug 09 18:03:28 EDT 1999 | Earl Moon
| | I am having cleaning problems when processing PCB's which have | | TAIYO solder mask on them. After processing, hand soldering and | | cleaning, a sticky residue is remains, resulting in a cosmetically poor finish with tide marks etc. Other solde
Electronics Forum | Wed Mar 10 17:03:52 EST 1999 | Morziana Hasan
NASA CommQuest Photopolymerized Conducting Polymers Directions: 1.Please read the information provided on this technology. You may follow the links to additional information resources below. 2.After evaluating the technology, please answer the
Electronics Forum | Tue Aug 10 16:01:12 EDT 1999 | Earl Moon
| | | | | | I am having cleaning problems when processing PCB's which have | | | | | | TAIYO solder mask on them. After processing, hand soldering and | | | | | | cleaning, a sticky residue is remains, resulting in a cosmetically poor finish with tid
Electronics Forum | Tue Aug 10 07:28:49 EDT 1999 | Brian
| | | I am having cleaning problems when processing PCB's which have | | | TAIYO solder mask on them. After processing, hand soldering and | | | cleaning, a sticky residue is remains, resulting in a cosmetically poor finish with tide marks etc. Other
Electronics Forum | Tue Aug 10 15:19:55 EDT 1999 | Earl Moon
| | | | I am having cleaning problems when processing PCB's which have | | | | TAIYO solder mask on them. After processing, hand soldering and | | | | cleaning, a sticky residue is remains, resulting in a cosmetically poor finish with tide marks etc.
Electronics Forum | Tue Aug 10 15:47:34 EDT 1999 | John Thorup
| | | | | I am having cleaning problems when processing PCB's which have | | | | | TAIYO solder mask on them. After processing, hand soldering and | | | | | cleaning, a sticky residue is remains, resulting in a cosmetically poor finish with tide mark
Electronics Forum | Thu Mar 11 10:31:57 EST 1999 | Justin Medernach
| NASA CommQuest | | | Photopolymerized Conducting Polymers | | Directions: | 1.Please read the information provided on this technology. You may follow the links to additional information resources below. | | 2.After evaluating the technology,
Electronics Forum | Mon Mar 22 18:03:15 EST 1999 | Marc
| | | | | Hi folks, | | | | | | | | | | I am looking for inputs on a long-standing problem encountered in our shop: Bottom-side parts (passives) falling off in the Wave...where the only remnants of the part is a flattened glue dot of proper diamet