Electronics Forum | Thu Nov 30 09:51:53 EST 2006 | Loco
Thanks for the replies, it is getting clearer now. We called a PCB supplier and acted if we didnt know what was what, he actually told us its all the same, chemical, flash, immersion, all the same... It is now getting clearer why we are sometimes ge
Electronics Forum | Thu Sep 10 15:01:28 EDT 2009 | mefloump
I currently spray DOW 2620 with my PVA650 without any problems. I do not thin it but I do have a distance between the coating machine and IR oven to provide a flash off period. I notice bubbles only when the flash off time is too short and the coatin
Electronics Forum | Wed Aug 19 03:24:49 EDT 2015 | pcbman
I ordered few times of prototyping gold plating > pcb from China. How to i differentiate they are > ENIG or Flash gold? Hi,Friend , this is very easy to distinguish the ENIG and gold plating pcb, you can stratch the solder mask off and see the co
Electronics Forum | Tue Mar 13 20:47:39 EDT 2018 | davef
I think of palladium coated copper with gold flash (CuPdAu) as bond wire used in chip attach. Look here: https://www.heraeus.com/media/media/het/doc_het/products_and_solutions_het_documents/bonding_wires_documents/fact_sheets/Factsheet_PdFlash.pdf
Electronics Forum | Tue Feb 01 21:51:05 EST 2000 | Dave F
Roni: Ron gives good advice on the thickness of your Electroless Nickel - Immersion Gold (ENIG) solderability preservative. Several additional comments are ENIG: � More expensive than OSPs and HASL. � Much flatter surface than HASL, similar to OSP
Electronics Forum | Thu Dec 08 01:05:34 EST 2005 | Mike_Kennedy
Our new PCB supplier can give us a 20% price reduction if we convert from an ENIG finish to a FLASH gold finish. My uderstanding between the two is as follows: ENIG - Nickel is plated over copper and then immersed in Gold which forms a self limited f
Electronics Forum | Tue Nov 28 17:23:03 EST 2006 | flipit
Flash gold usually refers to electrolytic gold with a short plating time. In other words gold plating that requires current to plate. If you have bare copper under your soldermask, the gold is probably ENIG. The only other way to have bare copper
Electronics Forum | Tue Nov 09 21:20:28 EST 1999 | Gyver
Hello all, Recently, we had a bad problem of block protection. You know, our programmer can't protect the 29F002 flash ROM, and our motherboard doesn't have 12 volts output for BIOS. So, from the preceding phenomena, it seems impossible to get a prot
Electronics Forum | Sat Feb 28 21:33:30 EST 1998 | P.L. Sorenson - Technical Consultant
| We are from Brazil and looking for a special kind of microchips: | Encapsulated microchip, battery operated, that drive 1 or 2 LEDs (light | emissor diode) to blink (JUST AN OSCILATOR). | (like the ones used in promotional musical CD box). we need,
Electronics Forum | Thu Mar 30 08:38:58 EST 2006 | Dan
We have this panel that is Gold Flash. Am I correct in assuming this is technically a lead-free panel then? We are running a WS paste, and the QFN28 has balls of solder instead of a fillet. My Max temp is 216, and the TAL was between 52-57 secs with