Electronics Forum | Mon Dec 22 10:24:06 EST 2008 | ck_the_flip
Yes I agree with Emil that the Jig/Fixture design is crucial for alignment. The hot-bar machine I worked with came with a digital camera and monitor to aid with alignment. Other than that, the right profile (heat, pressure and dwell), and a good fl
Electronics Forum | Fri Jan 10 11:36:03 EST 2014 | rgduval
One thing you could check/monitor is the temperature in the pot/wave. As boards run across the wave, they will cause fluctuations in the wave temperature. The heaters should hep with minimizing this; but, if you're running a lot of boards in quick
Electronics Forum | Wed Dec 22 14:21:13 EST 2004 | James Dornan of APE Inc
A little late but if this subject is still of interest the following paper from APE may be of interestwhen considering IR to Air Bath: HOT AIR versus IR and other convection Rework Systems HOT AIR is the most popularly chosen method of rework in th
Electronics Forum | Fri Mar 21 15:51:23 EDT 2008 | g2garyg2
Thought I would reply and try to assist. PROMATION, my company, also manufactures Diode Laser soldering systems but with this stated we also manufacturer iron tip systems, soft beam systems and hot air solutions. The reasons are simple. Diode Laser
Electronics Forum | Mon Nov 09 09:44:22 EST 2015 | davef
Purpose. This describes setting-up a wave soldering system set-up for a new assembly design or checking a wave solder machine operation with a test board. Applicability. To be used for new design printed circuit assembles and during machine accept
Electronics Forum | Fri Jul 30 17:13:30 EDT 1999 | Dave F
| | | Looking for solder paste specification limits which have reliability data to support them. Currently, we are looking to define the min/max volume necessary to ensure a good joint on CBGA, PBGA, and Micro-BGA's. Any information will be greatly
Electronics Forum | Mon Aug 17 02:50:44 EDT 1998 | Bob Willis
| Have an SRT w/preheat, 18 layer board all copper, 456 BGA needs to be removed and replaced. The manufacturer is Chip Express and during reflow it warps up or down. Causing either opens or shorts on the corners. I was using gel flux with multiple