Electronics Forum | Fri Sep 08 12:03:24 EDT 2017 | rameshraja
Hi, I need the RF 800 Flux Acid titration procedure and also require EPT of the same to add thinner ( RF 800 additive), i.e we are using the flux rf 800 for our wave soldering process having foam fluxer , after 2 hours we are taking sample from the
Electronics Forum | Wed May 27 15:09:30 EDT 1998 | Dave F
| | | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not locali
Electronics Forum | Tue Nov 03 16:28:21 EST 1998 | Dave F
| Well my process is I'm running my belt speed at 3.50fpm and about 215 to 225 degrees top side. I got my main wave down to a little less than half the board thickness. I'm not using a hot air knife cause we thought it might create more of a problem
Electronics Forum | Wed May 27 09:56:39 EDT 1998 | Chrys
| | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not localize
Electronics Forum | Wed May 27 15:54:09 EDT 1998 | Chrys
| | | | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not loca