Electronics Forum | Tue Oct 31 22:56:23 EST 2006 | davef
So at incoming inspection, what are the results for your "dip & look" solderability testing [IPC/JEDEC J-STD-002A] of the specific problem component?
Electronics Forum | Wed Dec 11 06:47:33 EST 2019 | ameenullakhan
Dear Friends, Need your valuable feedback on how to identify the component is ok or not for manufacturing. Issue : We have parts which are more than 5 years old.And management want us to qualify this parts for production. We presently use below me
Electronics Forum | Tue Sep 12 19:36:17 EDT 2006 | davef
We've been soldering leadfree components for maybe 15 years. We'd be surprised not to be able to store components for at least a year, not that we purposely do that. Component fabricator process determine the maximum storage time for components. M