Electronics Forum | Fri Oct 08 17:12:31 EDT 1999 | Dave F
| Hi, | | Does anybody know what is the minimum gold plating thickness on the PCB goldfinger required by the industrial specifications - IPC, Bellcore, etc. Where can I find the information? Appreciate for the help! | | Thanks, | Tony | Hi Tony:
Electronics Forum | Thu Oct 07 20:34:48 EDT 1999 | Tony Huang
Hi, Does anybody know what is the minimum gold plating thickness on the PCB goldfinger required by the industrial specifications - IPC, Bellcore, etc. Where can I find the information? Appreciate for the help! Thanks, Tony
Electronics Forum | Tue Apr 17 21:30:27 EDT 2001 | davef
The issue is on the table. Which is it? Are you ... * Loosing your gold plate when you remove the tape? [A tape test is a standard test for evaluating gold fingers. Check IPC-TM-650, test number wachacallit. Checkitaut.] OR * Putting tape o
Electronics Forum | Wed Aug 11 18:36:03 EDT 2004 | davef
90 Knoop. Q2: Thickness is 4 to 10 u" for Au and 300 to 400 u" for nickel A2: This looks like a ENIG spec. Although, the Ni is quite heavy, 150 uin is sufficient for most applications. [IPC-4552 ENIG specification: * Gold thickness of 0.075 - 0.125
Electronics Forum | Fri Jan 06 00:03:10 EST 2023 | SMTA-64419298
Hello Evtimov, sorry...just saw post as I was looking through list...a bit late. I don't know if you ever got your answer. IPC-4552A covers EniG finishes and suggested shelf life. I've referred to these doc's quite a bit. Good spec's ! Yes, I beli
Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty
| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec
Electronics Forum | Tue Dec 01 09:02:18 EST 1998 | Earl Moon
| | | Hi folks , | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our in
Electronics Forum | Fri Dec 04 20:26:34 EST 1998 | kallol Chakraborty
| | | | Hi folks , | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Ou
Electronics Forum | Fri Dec 04 20:37:45 EST 1998 | kallol chakraborty
| | | | | Hi folks , | | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most
Electronics Forum | Fri Nov 13 23:33:33 EST 1998 | Kallol Chakraborty
| | | I believe that gold fingers on my circuit boards are being | | | contaminated and need to clean them with some chemical | | | solution. Any recommendations. | | | | | Chuck: What is the type and source of your contamination? Dave F | | We a
IPC is the trade association for the printed wiring board and electronics assembly industries.
Training Provider / Events Organizer / Association / Non-Profit
3000 Lakeside Drive, 309 S
Bannockburn, IL USA
Phone: 847-615-7100