Silicon contamination in solder joint

Electronics Forum | Wed May 28 14:35:47 EDT 2003 | davef

Wow, you're very correct. I guess we use silicone to calibrate our machine, as follows: XPS spectral measurements of dimethyl silicone should include O(2s) at 25 eV, Si(2p) at 102 eV, Si(2s) at 153 eV, C(1s) at 285 eV, and O(1s) at 533 eV. The C(1s

Kenco Industries Ionic Tester

Electronics Forum | Sat Jun 25 19:35:31 EDT 2005 | Mike Konrad

The Kenco ionic contamination tester (Zero-Ion) is now manufactured and supported by Aqueous Technologies. www.aqueoustech.com service@aqueoustech.com (909) 944-7771 Mike Konrad

Ionic Contamination Tester

Electronics Forum | Wed May 14 20:33:52 EDT 2008 | davef

1 DYNAMIC TESTERS * Kenco ionic contamination tester (Zero-Ion) [Aqueous Technologies; http://www.aqueoustech.com 909-944-7771 Mike Konrad * Ionograph [Specialty Coating Systems; 7645 Woodland Dr, Indianapolis, IN, 46278; 800-356-8260 317-244-1200 F3

Calculating PCB surface area

Electronics Forum | Fri May 17 03:04:15 EDT 2002 | Mike Konrad

This conversation reminds me of the old �How Many Engineers Does It Take To�� joke. We manufacturer the ionic contamination (ROSE, SEC) testers and I am not aware of anyone that performs such exacting surface area calculations. Most people use th

IONIC CLEANLINESS SPEC FOR BARE PWBs

Electronics Forum | Fri Dec 06 12:24:03 EST 2002 | Mike Konrad

Military and most commercial standards requires post-soldered boards to measure less than 10 �g/in of NaCl (14 when using an Omegameter, 20 on a Ionagraph, and 37 on a Zero-Ion). As Dave stated, 6.5 �g/in of NaCl is called out in Mil-P-55110 for ba

IONIC CLEANLINESS SPEC FOR BARE PWBs

Electronics Forum | Sun May 09 16:25:00 EDT 2004 | gabriele

Military and most commercial standards requires > post-soldered boards to measure less than 10 > �g/in of NaCl (14 when using an Omegameter, 20 > on a Ionagraph, and 37 on a Zero-Ion). > > As Dave > stated, 6.5 �g/in of NaCl is called out in >

Calculating PCB surface area

Electronics Forum | Tue May 14 08:04:58 EDT 2002 | robbied

Hi. Does anyone out there know of a way to calculate the surface area of populated PCB's? We build many different types, and until now have been using a water displacement method, which I believe to be fundamentally flawed. Our technique is to drop a

Re: Cleanliness Testing/Conformal Coating

Electronics Forum | Tue May 11 07:50:52 EDT 1999 | Graham Naisbitt

| If I clean my assembly and find no visable contamination with the unaided eye, do I need to do cleanliness testing prior to conformal coating? | Douglas, It is highly advisable to test for ionic contaminants because a coating seals in as well as

Re: Zero-Ion Ionic Tester

Electronics Forum | Wed Feb 02 12:11:31 EST 2000 | Dave F

Casimir: Resistivity of Solvent Extract (ROSE) testers measure ionic contamination by washing boards with a DI water/IPA solution. (No-clean people: Stop and go on to something else.) The testers are process control instruments used to monitor a

Changing a wave over to lead free

Electronics Forum | Thu May 18 14:50:08 EDT 2006 | grantp

Hi, The bath is titanium coated, and the machine is only 2 years old, and was designed for lead free, so we know we don't need to change anything. The reason the supplier gave for suggesting the bath change is "other companies are doing it" and it'

  1 2 Next

kenco contamination calculator searches for Companies, Equipment, Machines, Suppliers & Information

Selective soldering solutions with Jade soldering machine

Wave Soldering 101 Training Course
Selective soldering solutions with Jade soldering machine

High Precision Fluid Dispensers
SMTAI 2024 - SMTA International

World's Best Reflow Oven Customizable for Unique Applications