Electronics Forum | Wed Mar 31 09:05:36 EST 2004 | russ
That would be one BIG spreadsheet, there are a lot of mfg with a lot of components for each one. As you know when going to the datasheetlocator you notice the huge listing of suppliers (500+) each one of them probbaly has anywhere from 1 type of co
Electronics Forum | Mon Apr 05 13:23:07 EDT 2004 | Ron W
Low-consumption Nitrogen configurations with an on-board O2 analyzer is the ideal way to go. I cannot speak for all oven manufacturers, but ours have N2 fed to the reflow zone only, which to me is really only where you need it. The gauges/flowmeters
Electronics Forum | Fri Sep 15 12:37:37 EDT 2006 | Doug at AccuAssembly
I wanted to update some information on BarTector posted earlier. Brock Electronics stopped handling the BarTector product in Jan 2006. Our company, AccuAssembly, currently manufactures, sells and supports BarTector. For more information on what Bar
Electronics Forum | Wed Apr 07 08:28:41 EDT 2004 | Dougie
Hi, We are Scottish manufacturing company considering a move to Immersion Silver finished PWB's from HASL. The driver behind it being the RoHS and WEEE legislation in Europe at present. My question is... We plan on using a Sn/Cu/Ni solder bar in o
Electronics Forum | Wed Apr 07 08:30:22 EDT 2004 | Dougie
Hi, We are Scottish manufacturing company considering a move to Immersion Silver finished PWB's from HASL. The driver behind it being the RoHS and WEEE legislation in Europe at present. My question is... We plan on using a Sn/Cu/Ni solder bar in o
Electronics Forum | Mon Apr 12 08:10:17 EDT 2004 | wgaffubar
We are sometimes, not always, seeing very large voids in the solder joints of BGA's with Via in Pad. Some lots of PCB will have the voids and other lots of boards will not. I feel the via's are outgassing during reflow, due to the PCB not having been
Electronics Forum | Mon Apr 12 11:32:47 EDT 2004 | Luis Lazcano
Can you share some information on the hazardous materials and cleaning details for your manufacturing processes, please ? These are the questions I need to ask you: 1. Do you use brominated fire retardant in PWB material? If not, what other type
Electronics Forum | Thu Apr 22 10:43:25 EDT 2004 | tigerlordgm
We had a great deal of trouble cleaning adhesive residue from stencils using an alcohol stencil washer. Same kind of thing, adhesive build-up in aperture corners. The solution we came up with was to convert our stencil washer to run Zestron ES200, a
Electronics Forum | Wed Apr 21 10:37:34 EDT 2004 | russ
Only the manufacturer of this part can tell you if subjecting the entire assembly through reflow temps is okay. It is not a good assumption that "if a part can be hand soldered it can withstand reflow" there are many connectors/headers/buzzers/etc
Electronics Forum | Mon Apr 26 17:05:36 EDT 2004 | babe
If you have deep pockets and wish to spend alot of money over the next few years, then yes, call Metcal. Whatever solder iron you plan to use, it is my suggestion that you take a look at the board that you are going to solder. How big are the pads? H