Electronics Forum: matte tinning (Page 1 of 4)

Matte tin finish

Electronics Forum | Wed Aug 04 16:49:24 EDT 2004 | jim_bob

Regarding Lead Free component finishes, vendors are zeroing in on matte tin plating as the finish of choice. What test are performed, to determine if a finish is "matte" type (vs. non-matte)?

Matte Tin finish on sockets

Electronics Forum | Tue May 16 16:36:18 EDT 2006 | dougm

Has anyone had issues with chips not making a reliable connection in sockets with a matte tin finish (RoHS compatible)? We have had issues with these types of sockets. I sent some to the manufacturer, and was told there weren't any problems. We re

Intrusive reflow component selection

Electronics Forum | Mon Jul 10 09:23:47 EDT 2006 | Rob

Hi Dougs, Info as follows: TAICOM TSD42: Matte Tin, 240C for 5 secs TAICOM TSD08: Matte Tin, 225/3 secs (I wouldn't!) TAICOM TKB06MSL: Matte Tin 260/40 secs (TBC) HARTING 09232486824: Harting don't supply. TAICOM TI40BHS: Matte Tin, 225/3 secs (I

Tin

Electronics Forum | Wed Dec 21 21:24:59 EST 2005 | davef

Primary differences between Matte Tin plating and Bright Tin plating are: * Temperature compatibility ** Matte Tin is compatible with the elevated temperatures of lead-free, reflow processing (250-260C). ** Bright Tin has a tendency to discolor (turn

Matte tin finish

Electronics Forum | Thu Aug 05 14:45:03 EDT 2004 | davef

Bright vs matte tin is fairly easy, but there's a s whole bunch of alternatives, beyond those two choices. So, no, not that we know.

Tin

Electronics Forum | Wed Dec 21 10:59:44 EST 2005 | Dhanish

1)What is the difference between Bright and Matte Tin? 2)How do you perform Tin Whisker Test?

Matte Tin finish on sockets

Electronics Forum | Tue May 16 18:05:05 EDT 2006 | russ

Need to switch from tin to possibly gold contacts, tin oxidises. Russ

Propensity of Immersion Tin surface finish fo whiskers

Electronics Forum | Mon Dec 12 11:18:59 EST 2005 | muse95

OK, I feel the need to jump in here. Bright Tin has the tendency to easily whisker, and is almost never used, except on some through-hole connectors, I believe. Matte Tin is much less susceptible to whiskering, although under the right stress cond

Matte tin finish

Electronics Forum | Wed Aug 04 18:38:53 EDT 2004 | davef

whiskers / "matte" => no whiskers. Look here: http://nepp.nasa.gov/whisker/anecdote/20year/ There. Nice going. What a buzz killer. I've got to got find some donuts, cold pizza, er whatever.

Matte tin finish

Electronics Forum | Thu Aug 05 10:55:19 EDT 2004 | jim_bob

Thanks. Yes, this is a interesting topic, and one that keeps our component engineers busy these days. I'm familiar with the data you referenced. Is there a "easy" method (test method) to use at incoming inspection to verify a termination is "matte

  1 2 3 4 Next

matte tinning searches for Companies, Equipment, Machines, Suppliers & Information

SMT feeders

High Precision Fluid Dispensers
Gordon Brothers October 2-30, 2024 Auction

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
Voidless Reflow Soldering

Reflow Soldering 101 Training Course
High Throughput Reflow Oven

Stencil Printing 101 Training Course
Hot selling SMT spare parts and professional SMT machine solutions

Private label coffee for your company - your logo & message on each bag!