Electronics Forum: non activated rosin flux (Page 1 of 10)

Mixing no-clean solder with activated

Electronics Forum | Tue Jun 26 19:51:31 EDT 2001 | davef

Rosin. A hard, natural resin, consisting of abietic acid [and pimaric acids in Europe] and their isomers, some fatty acids, and terepene hydrocarbons. Rosin is extracted from pine tree stumps. It�s an organic material distilled from oleoresin in p

Mixing no-clean solder with activated

Electronics Forum | Mon Jun 25 20:35:44 EDT 2001 | davef

According to J-STD-004 "Requirements for Soldering Fluxes", fluxes are classified by their chemical composition, activity level and halide content. In this scheme, each flux type is identified by a 4-character designator, where: * First two character

Mixing no-clean solder with activated

Electronics Forum | Tue Jun 26 10:49:59 EDT 2001 | genny

Yes I have read that standard, but it doesn't tell me what I need to know. Both have the same activity level and halide rating (L0) The AIM technical guy told me RO is a natural gum rosin, while (RE) Resin has more processing or something (maybe so

Mixing no-clean solder with activated

Electronics Forum | Wed Jun 20 11:28:45 EDT 2001 | Steve

Fluxes that have been properly heat activated are insulative (non-reactive) during operation in the field and during environmental testing. If you are also performing a cleaning operation, the possibility of growing dendrites is so remote that it can

clean process vs non clean process

Electronics Forum | Fri Apr 02 00:16:18 EST 2004 | Mike Konrad

There is no shortage of reasons to clean your boards. Soldering or reflowing your boards leaves �stuff� on them. This �stuff� is normally corrosive and conductive (some fluxes / pastes are more corrosive / conductive than others). In either case,

no-clean flux vs. impedance

Electronics Forum | Mon Feb 18 17:36:32 EST 2008 | kennyg

I should have mentioned... the only flux we use for the hand soldering is wire-core, no bottle flux. I think it should be a non-issue to leave the activated wire core flux residue. I'm just looking for some way to prove it to the designer.

"R" type solder paste

Electronics Forum | Thu May 11 11:25:56 EDT 2017 | davef

Key to Rosin Fluxes [from SUPERIOR FLUX & MFG. CO.] Type R (Rosin): Non-activated rosin flux for soldering copper. Residues are non-corrosive and non-conductive. Type RMA (Rosin Mildly Activated): Mildly activated rosin flux that contains no chlori

Re: When using noclean flux or clean flux process?

Electronics Forum | Tue Sep 21 13:10:10 EDT 1999 | Dave F

| Dear All, | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | I mean that I wonder why we use

flux on PCB's after cleaning

Electronics Forum | Fri Jul 23 14:41:41 EDT 2004 | Steve Stach

Dear JSK, It sounds like the root causes of your problem are two fold. First, excessive heat will polymerize the abietic acid found in rosin forming neo-abietic diamers and polymers which are much less soluble than the parent monomer. There are

Re: When using noclean flux or clean flux process?

Electronics Forum | Wed Sep 22 02:45:23 EDT 1999 | Brian

| | Dear All, | | | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | | | I mean that I wonder

  1 2 3 4 5 6 7 8 9 10 Next

non activated rosin flux searches for Companies, Equipment, Machines, Suppliers & Information

SMTAI 2024 - SMTA International

High Resolution Fast Speed Industrial Cameras.
Solder Paste Dispensing

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
Voidless Reflow Soldering

Software for SMT placement & AOI - Free Download.
High Throughput Reflow Oven

Training online, at your facility, or at one of our worldwide training centers"