Craig & Rem - I would also recomend switching to ENig - OSP would be my sencond choise ENig will give you the flatness your looking for plus the best shelf life. Enig is about 5% more than Hot Air. Enig also does not cause as much stress on the c
Electronics Forum | Sat Jun 30 11:28:24 EDT 2001 | davef
Consider using a roll solder with a flux that well matches the residues you can accept to be remaining on the board when you get finished processing. Many people use a no-clean flux cored roll solder for such operations, because they don't want to c
Electronics Forum | Tue Aug 09 11:57:11 EDT 2005 | Board House
Hi Ted, I am a Sales Manager for a Circuit board Manufacture in MN. We have seen the Majority of our Customer base switch to Enig do to shelf life issues of silver and Tin. Silver, Tin & OSP all have a shelf life between 6 - 8 Mos. Enig is betwee
Electronics Forum | Wed May 16 15:40:56 EDT 2012 | davef
Here's some notes from a Bob Willis presentation Assembly of Flexible Circuits with Lead-Free Solder Alloy [Bob Willis leadfreesoldering.com] * Flexible Circuit Construction ** Base Material - 0.05mm Copper 18/18 um ESPANEX from Holders Technologies
Electronics Forum | Thu Apr 22 06:42:03 EDT 2004 | Chris Lampron
Adam, What is the pad finish on the flex circuit? Is this the only component that you are having problems with? (on this Flex)If this is the only problem area on the flex (assuming there is more than one component)then that would lead me towards the
Electronics Forum | Mon Jul 22 15:02:31 EDT 2013 | dyoungquist
What is the pad surface finish on these boards? I know OSP and silver finishes have a shorter shelf life than HASL or gold. We do not use OSP or silver on our boards so I don't know what to look for visually on the pads when they have exceeded the
Electronics Forum | Thu Aug 25 11:53:12 EDT 2016 | shawn_halo_1
Sorry if I was not clear. We have a Flex Circuit Board that is ENIG Finished. There are two connectors that are SMTd to either side of the Flex to connect to other PCBs within the system. Then, we have conductive rubber contacts that are press fit on
Electronics Forum | Thu Feb 15 07:47:12 EST 2007 | zanolli
1" long SMT components to be placed without coplanarity issues> Also, what types of finishes are common for the flex;i.e, ENIG, immersion Ag, etc.?
Electronics Forum | Tue Sep 13 12:00:57 EDT 2011 | swag
Flex circuits are assemblies that can be bent or twisted into shapes after assembly (flexible). When heald in panels for SMT assembly, it's difficult to get repeated x/y offsets so you need to consider fiducal placement in your design for placment m
Electronics Forum | Wed Oct 10 16:16:15 EDT 2001 | lisa
Hello all, I'm looking for some advice on inter-metallic formation. I have some circuit board finished with Immersion Tin, Immersion Silver and OSP. They have been reflowed with solder past and components,the joints look good. What can I expect fo