Electronics Forum: osp flex (Page 1 of 1)

Re: Immersion Silver PCB Surface Plating

Electronics Forum | Wed Feb 02 20:53:34 EST 2000 | Dave F

Dennis: Several points: 1 If you're talking AlphaLevel process (?): � Good solderability, as HASL, even no-cleans bite well. � Planarity, uniform deposit, no bridgin� of FP. � Doesn't store as well as NiAu ... LT 6 months sealed � Very sensitive t

Lead Free ...

Electronics Forum | Thu Sep 02 10:24:35 EDT 2004 | dj_jago

Greetings from the UK: I have been quite fortunate to lead (no pun intended) our company towards lead free sooner rater than later. One of our customers produces a product which is refurbushed every 6 months or so and sent back into the market. A

Assemby of flexible printed circuits

Electronics Forum | Wed May 16 15:40:56 EDT 2012 | davef

Here's some notes from a Bob Willis presentation Assembly of Flexible Circuits with Lead-Free Solder Alloy [Bob Willis leadfreesoldering.com] * Flexible Circuit Construction ** Base Material - 0.05mm Copper 18/18 um ESPANEX from Holders Technologies

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 15:27:36 EDT 1998 | Dave F

| | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and s

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 20:18:09 EDT 1998 | Justin Medernach

| | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon

| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon

| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered

  1  

osp flex searches for Companies, Equipment, Machines, Suppliers & Information

pressure curing ovens

Training online, at your facility, or at one of our worldwide training centers"
2024 Eptac IPC Certification Training Schedule

High Resolution Fast Speed Industrial Cameras.
thru hole soldering and selective soldering needs

World's Best Reflow Oven Customizable for Unique Applications
Pillarhouse USA for Selective Soldering Needs

Component Placement 101 Training Course
Electronic Solutions R3