Electronics Forum | Wed Dec 10 10:05:07 EST 2003 | davef
We do not have experience soldering to the PVD surface you plan to use. We use Titanium [Ti] stiffeners in wave soldering and our wave equipment manufacturer uses Ti fingers, nozzles, pump blades, and other parts, because solder doesn�t stick to Ti.
Electronics Forum | Sat Jun 30 11:28:24 EDT 2001 | davef
Consider using a roll solder with a flux that well matches the residues you can accept to be remaining on the board when you get finished processing. Many people use a no-clean flux cored roll solder for such operations, because they don't want to c
Electronics Forum | Thu Aug 06 09:51:20 EDT 1998 | Bob Willis
This text may be of interest to any one with tin lead spots Guide to Solder Spots - A New Plague in Manufacture ? So what are solder spots ? They appear to be the next big problem in modern reflow assembly in fact in any process that involves solder
Electronics Forum | Sun Aug 29 19:17:34 EDT 2004 | aqueous
Chen, It is always best to place one�s effort on determining the cause and content of the residue rather than trying to work around it. The first thing you must determine is the nature of the residue. Is it flux? In many instances, the residue is
Electronics Forum | Sat Mar 01 16:46:26 EST 2003 | MA/NY DDave
Hi Hey thanks, you are welcome for the link. Well to be precise dissimilar metals will corrode at some rate and also depends on the environment. Look at a Galvanic Table. Yet maybe for your application and the ones AMP designed this part for, the c
Electronics Forum | Fri Mar 17 16:58:52 EST 2006 | mikecollier
We are currently struggling with a particularly difficult component selection form our designers. This is a custom BGA, 592 balls, metal cover with a very large bead of adhesive using to retain the cover. We have had significant fallout (greater th
Electronics Forum | Thu May 21 09:54:07 EDT 1998 | Justin Medernach
| I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and solde
Electronics Forum | Wed Jan 13 20:44:42 EST 1999 | Steve Gregory
Hello Sanjay! The cheap deal I use that Earl spoke of is called a SMarT Measure. It's a depth measuring microscope that uses the same principle of measuring optical focus that the units from Vision Engineering do ( if you've ever looked at any
Electronics Forum | Thu Jan 14 11:08:29 EST 1999 | Mike McMonagle
Steve, Whoa, take a breath! That was at least a dollar three-eighty answer. I've got to agree that nothing can replace a qualified, concientious operator for assuring quality. When I too worked at a small shop there in SillyCone Valley, my seni
Electronics Forum | Thu Jan 14 15:22:14 EST 1999 | Earl Moon
| Steve, | Whoa, take a breath! That was at least a dollar three-eighty answer. I've got to agree that nothing can replace a qualified, concientious operator for assuring quality. When I too worked at a small shop there in SillyCone Valley, my