Electronics Forum | Wed Jun 15 10:38:41 EDT 2016 | laynefelix
Hi everyone..i am new here. I am hardware design engineer and as per my experience PCBAs came out cold soldered after being reflowed the first time with ALPHA WS-820. The flux gel ALPHA WS 609 was supposed to be applied only onto the terminations of
Electronics Forum | Wed Oct 18 07:51:14 EDT 2006 | davef
Look here: http://www.circuittechctr.com/ As a low cost approach, use copper foil purchased from a stained glass window hobbyist shop. Cut foil pieces to size with a sharp knife. Epoxy the pieces in place of the damaged pads. Tin and then solder th
Electronics Forum | Mon May 21 17:32:23 EDT 2001 | davef
I said: "Our electronic circuit board fabricators seal the boards in moisture barrier bags [MBB]. We discontinued the use of desiccant bags in these MBB because of concerns about the desiccant releasing materials that would affect the solderability
Electronics Forum | Fri Apr 16 10:49:55 EDT 2010 | davef
Your picture is not very useful in conveying the stains. Could the stains be a delamination of the board?
Electronics Forum | Thu Apr 15 14:09:48 EDT 2010 | richardli
We found stains on the boards come out of reflow oven. The board itself color changed to yellowish from white . We understand discolor soldermask due to high temperature. This can be acceptable by our customer not the stains. The stains look like wa
Electronics Forum | Fri Apr 16 12:17:51 EDT 2010 | richardli
We have asked the supplier use whiter soldermask taking more heat. We also asked the board supplier to double coat board with soldermask. All these tries failed. We are wondering if the stains are flux contamination.
Electronics Forum | Thu Feb 14 17:40:34 EST 2013 | jorge_quijano
PCB Supplier made an EDX anaysis, the found a chemical trapped in the holes, and some burnt burrs, according to what they say this stains are over the solder mask & silk, so they do not affect functionality.
Electronics Forum | Wed Dec 19 01:17:13 EST 2001 | ianchan
Hi Experts, I need help here, advice appreciated from all... Production is running a Lot of flex-circuit PCB, through the SMT line, with 0402 components. The flex-PCB is taped to FR4 support "pallets" when processing thru' the SMT P&P m/c. We use
Electronics Forum | Fri Apr 16 11:51:26 EDT 2010 | shawnvike
Looks like a simple variance in the solder mask discoloring. Shawn
Electronics Forum | Wed Dec 19 02:24:40 EST 2001 | ianchan
Did I mention, we tried to use the same WS flux formulae to brush-cover the affected flex-PCB pads, and subject it to another round of water-wash, followed by oven-baking, and it still doesn't help abit? Oven bake : 100 deg-C, approx 15~30mins (manu
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830