raw copper on pcb

Electronics Forum | Thu Jun 07 05:11:42 EDT 2012 | cp38260

Hi, I have pcbs (Duroid/RT 5880) with raw copper, soldered in vapour-phase chamber at 230 degrees Celsius. During soldering, copper gets tarnished. Cleaning with Vigon A250 removes the tarnished layer. Indeed, in the VigonA250 techn. datasheet it is

pcb plating

Electronics Forum | Sun Sep 15 21:44:41 EDT 2002 | jason

Hi Dave, Immersion Ag has poor surface appearances after reflow or rather tarnished, while Immersion Tin requries higher temp. Probably that's why Immersion Ag is more preferred.

ALIVH pcb

Electronics Forum | Tue Apr 09 16:19:37 EDT 2002 | Peter L.

Has anyone built using the ALIVH PCB (0402, 0.8mm pitch uBGA) on the SMT line? I would like to know any process issues (paste printing, p&p, reflow) related to processing this pcb. Specifically, what type of solder paste was used (no clean) and wha

cleaning PCB's

Electronics Forum | Tue Jan 10 10:26:11 EST 2006 | mikeattekfab

I am considering using a vapor degreaser to clean PCB's after they emerge from our wave. Does anyone have experince with this process that they would be willing to share?

PCB cleaning

Electronics Forum | Sat Jun 12 17:01:44 EDT 1999 | Murray Pulman

We are using so called no-clean fluxws for our small batch production, however the results are not always very visualy pleasing with white powdery deposits being the norm. I would like advise on the best avenue to explore for a small batch cleaning s

cleaning PCB's

Electronics Forum | Tue Jan 10 14:34:40 EST 2006 | Amol Kane

arent there environmentally friendly solvents (i have seen some from 3M) that can be used in a vapor degreaser. i was also planning to use the vapor degreaser to clean boards prior to conformal coating

stencil cleaning

Electronics Forum | Tue Oct 11 10:49:14 EDT 2005 | jhagve

HI We start to make a product which have a 0.4 mm pitch IC and start having problems with not enough solder printed, to solve this problem we had to increase the manual cleaning, now we are cleaning the stencil every 8 printings, before we was runnin

Stencil cleaning

Electronics Forum | Tue May 30 10:55:57 EDT 2006 | bryanhewson

I am a lay person researching the application of non-woven material in stencil rolls either using branded material or non-branded alternatives for DEK, MPM Panasonic machines in SMT environments. I have read a number of articles referring to aqueous

cleaning PCB's

Electronics Forum | Tue Jan 10 14:04:38 EST 2006 | Mike Konrad

Flashback time� Vapor degreasers, although still used in limited applications, no longer represent the conventional wisdom (due to multiple environmental issues). Aqueous-based technologies are the most common method of defluxing. Unlike most va

cleaning PCB's

Electronics Forum | Tue Jan 10 20:39:06 EST 2006 | aqueous

Of course there are solvents which are less harmful to the environment than others. The operative phrase is �less harmful�. As a rule, water-based chemistries are �greener� than solvents. There are some solvent blends designed for aqueous-based eq

  1 2 3 4 5 6 7 8 9 10 Next

pcb cleaning tarnish. searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830

SMT Machines

High Throughput Reflow Oven
Win Source Online Electronic parts

World's Best Reflow Oven Customizable for Unique Applications
Software for SMT

We offer SMT Nozzles, feeders and spare parts globally. Find out more
Best SMT Reflow Oven

High Precision Fluid Dispensers