Electronics Forum | Mon Jan 29 17:45:35 EST 2001 | clem
The general guideline for most PCB manufacturers for PCB thickness tolerance is +/- 10%. Is this documented in an IPC spec? If so which one? Thanks Dave
Electronics Forum | Tue Jan 30 10:19:20 EST 2001 | ibi
I think that tolerance of pcb thickness is described in the �1-2-4 of IPC41-01 (Specification for Base Materials for Rigid and Multilayer Printed Boards Supercedes IPC-L-108, L-109, L-112, L-115, AM-361). Good reading,
Electronics Forum | Tue Nov 09 11:32:32 EST 1999 | Dave F
Wolfgang: "Our desire is to get what we design" ... Wanting to get what you ask for ... ummm sounds like a risky proposition!!! ;-) Two things: 1 Go to the Hadco site and get their "boiler-plate." Use it and some of the Earl Moon specs in the SMTn
Electronics Forum | Tue Nov 09 05:14:49 EST 1999 | Wolfgang Busko
Hi all, our problem we face is the mismatch of conductor width on the delivered PCB and the nominal width given by CAD-data. With CAD we are improving pads and conductors to match the specific needs for soldering and the board houses counteract our i
Electronics Forum | Thu Jun 09 07:02:02 EDT 2005 | ajaydoshi
1. We do have PCB with 0402 component, Micro BGA ( 0.5mm pitch , 0.25 mm pad size ). PCB thickness is 0.8mm. What stencil thickness we should use. PCB size 40 mm X 60 mm 2. We have EKRA E4 , What will be optimum setting for above. Pressure, Scquge s
Electronics Forum | Wed May 17 11:00:00 EDT 2000 | emmanuel
Has somebody yet process pcb (FR4) with a thickness of 0.8 mm ? Thank you for all kind of responses.
Electronics Forum | Fri Oct 03 07:49:18 EDT 2003 | mk
Mask Musings. Soldermask (SM) and its functions have changed and evolved over the years. As an ex-solder mask applicator, I can remember screening Colonial High Gloss Epoxy soldermask on boards back in the early 80's, ending up with a thickness that
Electronics Forum | Thu Jun 09 13:30:34 EDT 2005 | PWH
I would suggest 7mm thick "Durostone" as a carrier material. Cut lip/pocket for PCB so it is 0.05" thinner than thickness of PCB. Allow 0.010" gap on all sides of PCB. Machine lip to width between 0.050" and 0.100" to support under perimeter sides
Electronics Forum | Fri Feb 16 08:04:05 EST 2007 | GS
Hi, questions about PCB ImSn finishing : a) how much is the standard thickness (most common)? b) how much is the maximum thickness obtainable by this finishing process? Thank you Regards....GS
Electronics Forum | Thu Jun 09 07:36:49 EDT 2005 | ajaydoshi
Thanks, 1. Any idea how to go about pallet. because this PCB is single only ( not in multiple ). if you have some drawing / picture pl. send me at ajay_doshi@utlindia.com 2. What are other parameter to set on machine ajay
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830