Masking with hight temp non silicone tape before wave

Electronics Forum | Tue Feb 17 15:24:17 EST 2009 | glynnhamer

I know this is going to sound rather sad, but we have been using a Capton tape for years that contains silicone to mask large components as they go over the wave, as well as large plated holes on the pcb. It was handed down for years as accepted prac

Blowholes during wave soldering

Electronics Forum | Tue Aug 28 06:17:11 EDT 2007 | jgrootkoerkamp

I have problems with blowholes during the wave soldering process. I already find out that the stock time between reflow and wave is the most important. The longer the boards are in stock the more blowholes we have. We don't have a climat controlled

Pb-free wave soldering with SMD

Electronics Forum | Mon Nov 28 09:46:24 EST 2005 | pjc

I have waved gold (ENIG) boards. That's a pretty hot pot at 260C, wow. I have used 245C with good results. All other parameters look OK a glance. Well, PCB temp looks a little hot too at 130C before pot. 90-100C is typical for most No-Clean flux. At

Baking PCB's before Assembly

Electronics Forum | Thu Feb 24 14:58:11 EST 2000 | Greg denham

Does anyone have any information on baking boards to remove moisture before reflowing and waving assemblies? I've been told that we should do this to stop such problems as delamination of boards, blow holes, solder balls, etc. I don't know have any e

Baking PCB's before Assembly

Electronics Forum | Thu Feb 24 14:58:11 EST 2000 | Greg denham

Does anyone have any information on baking boards to remove moisture before reflowing and waving assemblies? I've been told that we should do this to stop such problems as delamination of boards, blow holes, solder balls, etc. I don't know have any e

Spray fluxing VOC free, as operation HOURS before wave solder

Electronics Forum | Wed Sep 20 10:36:27 EDT 2006 | proy

I am considering moving my spray fluxer into a completely separate operation. Has anybody any comments of sraying VOC free flux on boards, then putting them in a drier/holding rack for possibly say overnight, then running them through wave solder?

Spray fluxing VOC free, as operation HOURS before wave solder

Electronics Forum | Wed Sep 20 16:27:06 EDT 2006 | proy

As we are a low volume shop, the extra handling is not too much of a concern. My biggest concern is if the flux sitting on teh board for a long time (few hours) is going to cause any problems in solderability. My thought is that it should not as it

popcorning in wave soldering

Electronics Forum | Tue Sep 12 04:48:26 EDT 2000 | Daniel

Is there a risk of popcorning plastic components during wave soldering? (The PCB is first surface mounted, reflowed and washed. It is sometimes left in air environment for as long as 48 h before the throgh hole components are mounted and they are wa

0402 wave soldering

Electronics Forum | Wed Jan 14 06:41:08 EST 2009 | andrzej

I did not tried this before (never hada chance to do it) but I considered such option - maybe try using temporary wavesolder mask on such small components. Run both sides of PCB through SMT oven and then mask 0402 completely and go with wavesoldering

Blowholes during wave soldering

Electronics Forum | Thu Sep 06 17:37:05 EDT 2007 | hakerem

Hi Joris - There is an excellent wave solder guide called "Take No Prisoners" that includes instructions for attacking and eliminating solder balls and preventing their recurrence: 1. Increase Dwell Time Solder balls are normally caused by too much f

  1 2 3 4 5 6 7 8 9 10 Next

pcb time before wave soldering searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830

Software for SMT

High Precision Fluid Dispensers


High Throughput Reflow Oven
Void Free Reflow Soldering

Best Reflow Oven


SMT & PCB Equipment - MPM, DEK, Heller, Europlacer and more...