Electronics Forum | Thu Nov 02 17:15:34 EST 2000 | Erdem Bilaloglu
We are using semi-circular land pattern and 0.004" smaller appertures on screen. With stable rising slope (max:2.6degC/sec)we have not experienced any tombstonning so far.
Electronics Forum | Thu Apr 05 08:36:35 EDT 2001 | jmlasserre
use a solder join temperature of 200/210� whatever the pcb used (tin lead coated or osp or gold fash). 2nd ==> to adapt the temerature to the pcb used: - Reflow (200-210�) for tin lead coated pcb's (in this case we have just to reflow the solder
Electronics Forum | Mon May 16 18:03:30 EDT 2005 | davef
Key Issue: Will this machine solder your boards? You never know until you solder one. Any other avenues of analysis involve substantial risk. Flux Selection * High or low solids * VOC or VOC-free Solder Alloy * If using lead-free, avoid stainles
Electronics Forum | Sun Nov 08 15:27:25 EST 2015 | davef
Thinner: Flux thinner, NOT paint thinner We kept a spare stone in thinner in inventory. We cut PVC pipe to size, cap in one end, screw thread on the other, stone inside, filled with flux thinner and covered with a screw cap. I don't remember who we
1 |