Electronics Forum | Thu Jun 13 11:25:40 EDT 2002 | davef
Help us understand your situation by telling us about: * Is this a terminal-to-terminal short on a single MELF? Or is this a terminal-to-terminal short between or than one MELF? * Clearance of 0.8mm is the distance between what features? * Size ME
Electronics Forum | Fri Jun 14 14:25:05 EDT 2002 | davef
Good job clarifying things. So, your MELF are just rolling off the pads. So much for the rocket scientist that talked you into those �V� shaped apertures, eh? [Or taking it the other way: Wow, just think how bad it would be if they weren�t worki
Electronics Forum | Thu Dec 15 11:06:05 EST 2005 | Samir Nagaheenanajar
You might wanna try a small reduction in your stencil aperture. For example, for a 30-mil pad go 26-mil square aperture with 8 to 10-mil radius on your corners. Also, look at your designs. Is there enough resist between your pad and ball? Another
Electronics Forum | Wed Dec 14 23:32:19 EST 2005 | jhernan9
Hi, I'm having a lot of problems with BGA's shorts, we are using 0.005" stencil aperture 1 to 1 (0.014)", the paste is centre (I can not measured the height)was verified using electronic microscopie, the placement is centre (I'm using local fiducials
Electronics Forum | Wed Aug 29 05:30:30 EDT 2018 | teresat2
I guess these boards only used Fly test. Flying needle test is one of the methods to check the electrical function of PCB (short circuit test). The flight test machine is a system for testing PCB in a manufacturing environment. Instead of using the
Electronics Forum | Thu Jun 13 03:15:01 EDT 2002 | jkhiew
Hi Jax, After component placement, all melf diodes being checked & found no touching each other. Unfortunately, after reflow those MELFs are shorted.
Electronics Forum | Thu Jun 13 02:40:16 EDT 2002 | jax
Is the short apparent prior to reflow?
Electronics Forum | Wed Jun 12 22:35:03 EDT 2002 | jkhiew
We had alot of problem with melf diode short together after reflow soldering. The clearance is about 0.8mm & we used "v" shaped opening . PLease comment !
Electronics Forum | Thu Jun 13 05:46:34 EDT 2002 | jax
After reflow, Are the end terminals of the melf packages touching or is it a paste bridge? What type of reflow are you using? IR?... Convection?
Electronics Forum | Thu Jun 13 21:44:21 EDT 2002 | jkhiew
Hi all, * Defect : termial to terminal touching btw two melfs body that created short circuit. * Clearance : 0.8mm btw two melfs body. * Size melf : diameter=2.4mm to 2.7mm, length=4.8mm to 5.2mm * Stencil opening : "v" shaped to minimise component