Electronics Forum | Mon Mar 26 10:40:14 EDT 2007 | solderiron
WaveroomPlus can offer the following Sn95.5 Ag3 Cu0.7 Sn95.5 Ag4 Cu0.5 Sn96.5 Ag3.0 Cu0.5 Sn97 Ag2.5 Cu0.5 Steve@waveroomplus.com
Electronics Forum | Wed Nov 08 08:12:16 EST 2006 | jnaligan
hi... try evaluating eco solder paste Sn96.5/Ag3.0/Cu0.5 from Senju... output is good and i suggest your stencil's apperture ratio with the pad 1:1 when it comes to fine pitches...and BGA pads regards, janry
Electronics Forum | Wed Mar 12 08:03:30 EST 2003 | Surachai
Hi all Pls. help advise. Our board use RMA solder paste (Pb-free Sn96.5/Ag3.0/Cu0.5). Can we use No-clean paste flux (Delta 670S1) in rework process? If it can not be used, why?. Thanks very much for your advice. Surachai
Electronics Forum | Sat Nov 03 11:20:35 EDT 2012 | davef
EricR: There's substantial information about the properties of solder alloys on the web. Here's an example of something that I clipped from one site Alloy ||Solidus (°C)||Liquidus (C°) ||Tensile Strength (psi / MPa) Sn42 Bi58||-E-||138||8000 / 55.2
Electronics Forum | Sat Aug 22 15:12:32 EDT 2009 | rossi
Thank you for replying. 1) the finish is Gold Immersion (ENIG) 2) paste type EM907 SN96.5/AG3.0/CU0.5 3) it is always the same BGA but its not on the same ball every time. It is always at the joint on the PCB pad like the solder is not sticking prope
Electronics Forum | Mon May 17 16:34:25 EDT 2004 | pjc
I am an equip mfrs rep. I took a customer to my wave solder principal's factory to run their boards on a wave with no-Pb alloy, (Sn96.5 Ag3.0 Cu0.5) in air environment. The results were excellent with pot temp of 263C (505F). Their boards are low to