Electronics Forum | Thu Mar 04 20:05:47 EST 2004 | pdeuel
Russ, Thanks for the laugh. Glad to know some of you still have a sence of humor. I also could not figure out the reason for this thread. I will hadzard a guess that melting point of lead with aloy would not be diferant from melting point of lead by
Electronics Forum | Thu Dec 22 15:36:03 EST 2005 | CC
In general two step temperature reflow process requires minimum 40 deg C delta to be sucessful. We are not using vapor phase soldering but we have similar situation when we change to SAC lead free solder for PCB component population and secondary swe
Electronics Forum | Wed Nov 17 09:28:40 EST 1999 | Steve Z
Hello, I am new to the SMT area and I need to know what a "good" vapor phase reflow profile should look like. The fluids we are using have a BP of 45 C and 219 C. Thanks,
Electronics Forum | Thu Dec 22 12:05:37 EST 2005 | Tony
Currently we are using a 2 step vapor soldering process to manufacture our std. lead soldered parts. The first step was done with a ls240 vapor fluid and the second was done with a ls200 fluid. Using a 221 deg C sn95/Ag5 solder for the first step a
Electronics Forum | Fri Dec 08 21:36:42 EST 2000 | reg
Hi everyone!! I have less than one year in the US, and I had been working as a field smt engineer. I have almost two years of experience as a manufacturing engineer, but what I really would like to do is process engineering. Can somebody advice
Electronics Forum | Mon Jul 19 11:11:18 EDT 1999 | Wolfgang Busko
| Perhaps a little hard to find but is there anyone who uses a vapor phase process to solder populated card with BGAs. I am interested in the success rate of such a process. It is obvious that the throughput is reduce vs a convection oven but still t
Electronics Forum | Mon Jul 19 11:50:47 EDT 1999 | Mario
| | Hi, SMTASSY | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | First, we do not do real series produktion, only prototyping up to sometimes 20 uni
Electronics Forum | Mon Jul 19 12:37:15 EDT 1999 | Wolfgang Busko
| | | | | Hi, SMTASSY | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | First, we do not do real series produktion, only prototyping up to som
Electronics Forum | Tue Jul 20 05:29:14 EDT 1999 | Wolfgang Busko
| | | | | | | | Hi, SMTASSY | | | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | | First, we do not do real series produktion, only prototypi
Electronics Forum | Wed Mar 12 15:26:46 EDT 2014 | dan_ems
Hello, in my SMT process I have some problems with the solderability (look like dewetting) on a PCB with finish HASL Lead Free with a composition that is melt at 230 degree Celsius. My oven is with vapor phase and the peak temperature is 230 degre
Main Products: 1. Original new and Original Used SMT/AI Spare Parts. 2. SMT Equipments And Related Machine( SMT Calibration, SMT Feeder Carts,Conveyer etc.) 3. Maintenace and Repair Service Pre-Sales Service Provide details ab
Manufacturer's Representative / Manufacturer / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
3 Road Xintang, Fuhai Street,Fuyong
Shenzhen, 30 China
Phone: 13713862102