Electronics Forum: wetting on enig (Page 1 of 29)

No wetting on connector latches

Electronics Forum | Thu Sep 02 05:12:15 EDT 2004 | doi

I am using a triad connector and have problem with wetting at both connector latches.Observed that the leads have very good shiny wetting however concerning the latches the solder just seem to disappear to thin airafter reflow.The connector has a gui

No wetting on connector latches

Electronics Forum | Thu Sep 02 09:51:53 EDT 2004 | davef

We see latches from some suppliers that just are not solderable. Usually the nickel plate on the latch is poor, allowing the nickel to corrode, and requiring a more active flux [if you're lucky]. But lots of times, you end-up with partial wetting,

No wetting on connector latches

Electronics Forum | Fri Sep 03 04:04:19 EDT 2004 | doi

Thanks davef for a your insights :)

ENIG poor wetting

Electronics Forum | Mon Jul 29 18:59:08 EDT 2002 | davef

Stand-ups are a common problem with 0402. Search the fine SMTnet Archives to get started.

ENIG poor wetting

Electronics Forum | Wed Jul 31 17:35:16 EDT 2002 | davef

* Finally, when soldered by hand, do the problem pads take solder? Yes, the XRF analysis will be interesting.

ENIG poor wetting

Electronics Forum | Mon Jul 29 16:43:55 EDT 2002 | mcm4me

I have a customer with up to 8% scrap from one board supplier and 1% from another supplier for solder dewett and no wet over ENIG finish with mask defined pads. Initially I suspected mask residue on pads because of the no wets but I have come to find

ENIG poor wetting

Electronics Forum | Tue Jul 30 10:04:51 EDT 2002 | dason_c

Dave, I am very interesting to know about the dewetting or pull back, we are currently use the uP78 paste. Will nitrogen, profile setting help to reduce the dewetting. Thank.

ENIG poor wetting

Electronics Forum | Tue Jul 30 12:15:15 EDT 2002 | Rick Lathrop

Hi Dave, The paste applied to the board ends up on the tombstone. The pad has a thin covering of solder most of the time, this is why I think they call it a dewet. Occasionally the pad shows some areas of gold and very rarely are some pads not wet at

ENIG poor wetting

Electronics Forum | Thu Aug 01 08:58:47 EDT 2002 | Rick Lathrop

Good morning Dave F. I am not going to try to touchup the solder pad until I get surface analysis work done, don't want to ruin the evidence. I am getting XPS work done not XRF, XPS is X-ray Photoelectron Spectroscopy and can see very thin films of o

SN100C wetting problems

Electronics Forum | Fri Jul 13 12:32:14 EDT 2007 | rgduval

We've experienced this issue with SN100. A couple of things we've tried, all with varying levels of success: 1. Longer pre-heats. We use SN100 in a solder pot, and pre-heat the boards on our wave machine. This did have a positive effect, but I ne

  1 2 3 4 5 6 7 8 9 10 Next

wetting on enig searches for Companies, Equipment, Machines, Suppliers & Information

Count On Tools, Inc.
Count On Tools, Inc.

COT specializes in high quality SMT nozzles and consumables for pick and place machines. We provide special engineering design service of custom nozzles for those unique and odd components.

Manufacturer

2481 Hilton Drive
Gainesville, GA USA

Phone: (770) 538-0411