Electronics Forum: wire hole size[0] (Page 1 of 11)

Criteria for thermocouple wire attachment

Electronics Forum | Thu Dec 21 10:27:24 EST 2006 | realchunks

>>> Now you must take into account your total board mass as well. If you have tons of heat sinks, or parts on the other side that can affect your profile, you should have them on the board when profiling. That�s where the "engineering" part in all

Re: SMT repairs using wire links

Electronics Forum | Thu Sep 10 21:44:48 EDT 1998 | Steve Gregory

| I'll stop talking to myself and wonder how big Steve G is doing these days. | Earl Moon Hey Earl! I was wondering the same thing about you a few weeks back when we didn't hear much from you...but, I'm doing okay. Been busier than a one-legged

Re: SMT repairs using wire links

Electronics Forum | Fri Sep 11 09:36:04 EDT 1998 | Earl Moon

| | I'll stop talking to myself and wonder how big Steve G is doing these days. | | Earl Moon | Hey Earl! | I was wondering the same thing about you a few weeks back when we didn't hear much from you...but, I'm doing okay. Been busier than a one

Solder hole found after reflow

Electronics Forum | Tue Jul 18 21:48:15 EDT 2006 | davef

We assume by "solder hole" you mean void. We believe void formation is driven by the thermal recipe that you've chosen to use. Search the fine SMTnet Archives for further discussion. There is a tremendous amount of current industry discussion on v

PTH hole size for soldering wires

Electronics Forum | Thu Feb 05 05:27:55 EST 2004 | dszeto

We have recent customer asking for PCB's PTH hole size related to soldered wire AWG 18-26. Please kindly advise any international standard for captioned issue. Thanks!

PTH hole size for soldering wires

Electronics Forum | Thu Feb 05 08:39:16 EST 2004 | davef

IPC-2222 - Sectional Design Standard For Printed Board For Organic Printed Boards, Table 9-3 � Plated Through Hole Diameter To Lead Diameter Relationships will give you the standard information you require.

Through hole SMD in SMT process-Length question

Electronics Forum | Tue Jul 19 18:05:31 EDT 2016 | davef

I'm not real clear on what you're looking to understand, but let me get things started ... IPC-A-610F - Acceptability of Electronic Assemblies, 7.3.3 Supported Holes – Wire/Lead Protrusion Minimum length: You need to be able to discern the compone

ENIG (thru hole ring turns black after wave soldering)

Electronics Forum | Tue Aug 02 15:03:37 EDT 2016 | davef

On a previous black pad experience we soldered a wire to a fiducial and did a pull test to failure. On the black pad board the wire and solder pulled of clean leaving the fiducial on the board. On good boards the copper came off with the wire. If you

repairs on a through hole 4 layer board

Electronics Forum | Thu Jul 22 15:15:24 EDT 2004 | russ

You can purchase pad repair kits at some "radio shack" type stores or you can order them from some such as Circuit repair corp. If you know where the signal traces go from the individual connector pins I woul;d recommend just adding a wire frm the p

does copper wire become thinner when it dip to leadfree solder?

Electronics Forum | Wed Nov 02 21:58:17 EST 2005 | KEN

Copper wire will become thinner when dipped in tin/lead or lead free solder. The copper is disolved off of the bulk wire. This is one reason rework on solder pots must be restricted. Eventually, after repeated cycles you will have smaller and sma

  1 2 3 4 5 6 7 8 9 10 Next

wire hole size[0] searches for Companies, Equipment, Machines, Suppliers & Information

SMT Machines

High Throughput Reflow Oven
Win Source Online Electronic parts

World's Best Reflow Oven Customizable for Unique Applications
Software for SMT

We offer SMT Nozzles, feeders and spare parts globally. Find out more
Best SMT Reflow Oven

High Precision Fluid Dispensers