Technical Library | 2019-08-24 09:02:25.0
Many customers looking for IC shipping tubes value the appearance of the packing tube. They will feel that if the appearance of the IC tube does not look good, the quality will not be very good, so the first impression of the appearance of the Antistatic ic tube is very important. So what are the factors that affect the appearance of IC tubes?
Technical Library | 2013-01-18 02:42:14.0
ENIG (Electroless Nickel/Immersion Gold) is to deposit nickel gold plating which has good solderability, wear resistance , leveling appearance and small electric resistance. It included 4 steps that are pretreatment, immersion nickel, immersion gold and Post treatment...
Technical Library | 2009-03-19 20:23:54.0
Over the past several years, post-reflow defluxing of circuit assemblies has gained in popularity. Microminiaturization of components and boards, combined with higher expected reliability and increased product liability, have contributed to the prominence of defluxing. Lead-free solder paste - with its higher reflow temperatures and negative effects on flux - increase the likelihood of post-reflow defluxing to increase a product's reliability and aesthetic appearance.
Technical Library | 2007-04-18 19:23:22.0
Recent investigations have revealed that Pb-free solder joints may be fragile, prone to premature interfacial failure particularly under shock loading, as initially formed or tend to become so under moderate thermal aging. Depending on the solder pad surface finish, different mechanisms are clearly involved, but none of the commonly used surface finishes appear to be consistently immune to embrittlement processes. This is of obvious concern for products facing relatively high operating temperatures for protracted times and/or mechanical shock or strong vibrations in service.
Technical Library | 2008-09-04 17:57:24.0
In the quest for lower ESL devices, having the ESL reduced in the package is only half of the battle; connecting that device to the circuit determines how much of that low ESL appears to the circuit. For this low ESL part type, it would be a shame to take a part of 200 pH and add 2000 pH to its ESL because of via patterns on the PCB.
Technical Library | 2013-04-12 07:22:40.0
Here Chris talks about the pitfalls, the paucity of safe options for manufacturers seeking rare components, and his exasperation with organisations that appear to shelve common sense at the first sign of a shortage. He shares his ‘no nonsense’ approach to getting things right first time, and explains his thinking in establishing an independent distributor focused exclusively on delivering 100% component integrity.
Technical Library | 2014-03-27 14:50:01.0
Because of the phase out of CFC's and HCFC's, standard solder pastes and fluxes evolved from RA and RMA fluxes, to No-Clean, to low residue No-Clean, to very low residue No-Clean. Many companies came out with their cleaning solutions, aqueous and semi-aqueous, with each product release being more innovative than the previous one. Unfortunately for most of the suppliers of cleaners, two other trends appeared; lead-free soldering and the progressive miniaturization of electronic devices.
Technical Library | 2022-02-16 15:34:32.0
Because of the phase-out of CFCs and HCFCs, standard solder pastes and fluxes evolved from RA and RMA fluxes to No-Clean, to low residue No-Clean, to very low residue No-Clean. Many companies came out with their cleaning solutions, aqueous and semi-aqueous, with each product release being more innovative than the previous one. Unfortunately for most of the suppliers of cleaners, two other trends appeared; lead-free soldering and the progressive miniaturization of electronic devices
Technical Library | 2019-05-29 01:47:22.0
1.Vias near SMD pads: Solder can flow into the via after melted. As a result cold joint will appear in the end. Check the picture below. 2.Vias on SMD pads: Solder can flow into the via more easier after melted. Check the picture below. 3.Via opening without soldermask covered. When workers solder TH parts by hand, soldering iron can touch vias sometime, then tiny amounts molten solder will stay on vias. This can lead to electrical short easily. We recommend you make all vias tenting (covered by solder mask) if it is possible.
PCBNPI-Professional PCB Fab/PCB Assembly Service Provider From China
Technical Library | 2014-05-01 15:14:12.0
Bilayer graphene has been a subject of intense study in recent years. The interlayer registry between the layers can have dramatic effects on the electronic properties: for example, in the presence of a perpendicular electric field, a band gap appears in the electronic spectrum of so-called Bernal-stacked graphene. This band gap is intimately tied to a structural spontaneous symmetry breaking in bilayer graphene, where one of the graphene layers shifts by an atomic spacing with respect to the other. This shift can happen in multiple directions, resulting in multiple stacking domains with soliton-like structural boundaries between them