Technical Library: column grid array (Page 3 of 4)

Electromigration Damage Mechanics of Lead-Free Solder Joints Under Pulsed DC: A Computational Model

Technical Library | 2013-06-13 15:31:24.0

Electromigration (EM) is a mass transportation mechanism driven by electron wind force, thermal gradient, chemical potential and stress gradient. According to Moore’s law, number of transistors on integrated circuits (ICs) doubles approximately every 2 years. Moore’s law holds true since its introduction in 1970s. This insatiable demand for smaller ICs size, larger integration and higher Input/Output (IO) count of microelectronics has made ball grid array (BGA) the most promising connection type in electronic packaging industry. This trend, however, renders EM reliability of solders joints a major bottleneck to hinder further development of electronics industry...

Electronic Packaging Laboratory, State University of New York

Board-Level Thermal Cycling and Drop-Test Reliability of Large, Ultrathin Glass BGA Packages for Smart Mobile Applications

Technical Library | 2018-08-22 14:05:42.0

Glass substrates are emerging as a key alternative to silicon and conventional organic substrates for high-density and high-performance systems due to their outstanding dimensional stability, enabling sub-5-µm lithographic design rules, excellent electrical performance, and unique mechanical properties, key in achieving board-level reliability at body sizes larger than 15 × 15 mm2. This paper describes the first demonstration of the board-level reliability of such large, ultrathin glass ball grid array (BGA) packages directly mounted onto a system board, considering both their thermal cycling and drop-test performances.

Institute of Electrical and Electronics Engineers (IEEE)

iNEMI Pb-Free Alloy Characterization Project Report: Part II - Thermal Fatigue Results For Two Common Temperature Cycles

Technical Library | 2021-09-08 14:10:12.0

The Pb-Free Alloy Characterization Program sponsored by International Electronics Manufacturing Initiative (iNEMI) is conducting an extensive investigation using accelerated temperature cycling (ATC) to evaluate ball grid array (BGA) thermal fatigue performance of 12 commercial or developmental Sn based Pb-free solder alloys. This paper presents the initial findings from a specific subset of the temperature cycling test matrix. The focus is on comparing alloy performance for two of the most commonly specified temperature cycles, 0 to 100 °C and -40 to 125 °C.

iNEMI (International Electronics Manufacturing Initiative)

Lead-Free and Mixed Assembly Solder Joint Reliability Trends

Technical Library | 2022-10-31 17:30:40.0

This paper presents a quantitative analysis of solder joint reliability data for lead-free Sn-Ag-Cu (SAC) and mixed assembly (SnPb + SAC) circuit boards based on an extensive, but non-exhaustive, collection of thermal cycling test results. The assembled database covers life test results under multiple test conditions and for a variety of components: conventional SMT (LCCCs, resistors), Ball Grid Arrays, Chip Scale Packages (CSPs), wafer-level CSPs, and flip-chip assemblies with and without underfill. First-order life correlations are developed for SAC assemblies under thermal cycling conditions. The results of this analysis are put in perspective with the correlation of life test results for SnPb control assemblies. Fatigue life correlations show different slopes for SAC versus SnPb assemblies, suggesting opposite reliability trends under low or high stress conditions. The paper also presents an analysis of the effect of Pb contamination and board finish on lead-free solder joint reliability. Last, test data are presented to compare the life of mixed solder assemblies to that of standard SnPb assemblies for a wide variety of area-array components. The trend analysis compares the life of area-array assemblies with: 1) SAC balls and SAC or SnPb paste; 2) SnPb balls assembled with SAC or SnPb paste.

EPSI Inc.

Avoiding the Solder Void

Technical Library | 2013-02-08 22:56:47.0

Solder voiding is present in the majority solder joints and is generally accepted when the voids are small and the total void content is minimal. X-ray methods are the predominate method for solder void analysis but this method can be quite subjective for non grid array components due to the two dimensional aspects of X-ray images and software limitations. A novel method of making a copper "sandwich" to simulate under lead and under component environs during reflow has been developed and is discussed in detail. This method has enabled quantitative solder paste void analysis for lead free and specialty paste development and process refinement. Profile and paste storage effects on voiding are discussed. Additionally an optimal design and material selection from a solder void standpoint for a heat spreader on a BCC (Bumpered Chip Carrier) has been developed and is discussed.

Heraeus

The Last Will And Testament of the BGA Void

Technical Library | 2015-01-05 17:38:26.0

The impact of voiding on the solder joint integrity of ball grid arrays (BGAs)/chip scale packages (CSPs) can be a topic of lengthy and energetic discussion. Detailed industry investigations have shown that voids have little effect on solder joint integrity unless they fall into specific location/geometry configurations. These investigations have focused on thermal cycle testing at 0°C-100°C, which is typically used to evaluate commercial electronic products. This paper documents an investigation to determine the impact of voids in BGA and CSP components using thermal cycle testing (-55°C to +125°C) in accordance with the IPC-9701 specification for tin/lead solder alloys. This temperature range is more typical of military and other high performance product use environments. A proposed BGA void requirement revision for the IPC-JSTD-001 specification will be extracted from the results analysis.

Rockwell Collins

Room Temperature Fast Flow Reworkable Underfill For LGA

Technical Library | 2016-10-03 08:28:47.0

With the miniaturization of electronic device, Land Grid Array (LGA) or QFN has been widely used in consumer electronic products. However there is only 20-30 microns gap left between LGA and the substrate, it is very difficult for capillary underfill to flow into the large LGA component at room temperature. Insufficient underfilling will lead to the loss of quality control and the poor reliability issue. In order to resolve these issues, a room temperature fast flow reworkable underfill has been successfully developed with excellent flowability. The underfill can flow into 20 microns gap and complete the flow of 15mm distance for about 30 seconds at room temperature. The curing behavior, storage, thermal cycling performance and reworkability will be discussed in details in this paper.

YINCAE Advanced Materials, LLC.

Evaluation, Selection and Qualification of Replacement Reworkable Underfill Materials

Technical Library | 2019-02-27 15:23:47.0

A study was performed to investigate, evaluate and qualify new reworkable underfill materials to be used primarily with ball grid arrays (BGAs), Leadless SMT devices, QFNs, connectors and passive devices to improve reliability. The supplier of the sole source, currently used underfill, has indicated they may discontinue its manufacture in the near future. The current underfill material is used on numerous circuit card assemblies (CCAs) at several sites and across multiple programs/business areas. In addition, it is used by several of our contract CCA suppliers.The study objectives include evaluation of material properties for down select, dispensability and rework evaluation for further down select, accelerated life testing for final selection and qualification; and process development to implement into production and at our CCA suppliers. The paper will describe the approach used, material property test results and general findings relative to process characteristics and rework ability.

Northrop Grumman Corporation

Common Process Defect Identification of QFN Packages

Technical Library | 2019-07-23 22:33:47.0

The Quad Flat Pack No Leads (QFN) style of leadless packaging [also known as a Land Grid Array (LGA)] is rapidly increasing in us e for wireless, automotive, telecom and many other areas becaus e of its low cost, low stand-off height and excellent thermal and electri cal properties. With the implementation of any new package type, there is always a learning curve for its use in design and processing as well as for the Process and Quality Engineers who have to get to grips with the challenges that these packages bring. Therefore, this paper will provide examples of the common process defects that can be seen with QFNs /LGAs when using optical and x-ray inspection as part of manufacturing quality control. Results of trials conducted on four PCB finishes and using vapour phase and convection reflow will be discussed.

Nordson DAGE

Via In Pad - Conductive Fill or Non-Conductive Fill?

Technical Library | 2020-07-15 18:29:34.0

In the early 2000s the first fine-pitch ball grid array devices became popular with designers looking to pack as much horsepower into as small a space as possible. "Smaller is better" became the rule and with that the mechanical drilling world became severely impacted by available drill bit sizes, aspect ratios, and plating methodologies. First of all, the diameter of the drill needed to be in the 0.006" or smaller range due to the reduction of pad size and spacing pitch. Secondly, the aspect ratio (depth to diameter) became limited by drill flute length, positional accuracy, rigidity of the tools (to prevent breakage), and the throwing power of acid copper plating systems. And lastly, the plating needed to close up the hole as much as possible, which led to problems with voiding, incomplete fill, and gas/solution entrapment.

Advanced Circuits


column grid array searches for Companies, Equipment, Machines, Suppliers & Information