Technical Library: kester no clean (Page 1 of 1)

Characterization of No Clean Solderpaste Residues: The Relationship to In-Circuit Testing

Technical Library | 1999-05-07 11:24:21.0

Many manufacturers have now completed the conversion to no clean solder paste. Many factors governed this initial conversion, among those being cosmetics, solder ability, and process ability. In circuit testing or probing through no clean solder paste residues has topically not been a major factor in the conversion decision for several reasons. Due to board design, solder paste was only used on one side of the board and not subjected to testing...

Kester

WHY CLEAN A NO-CLEAN FLUX

Technical Library | 2020-11-04 17:57:41.0

Residues present on circuit boards can cause leakage currents if not controlled and monitored. How "Clean is Clean" is neither easy nor cheap to determine. Most OEMs use analytical methods to assess the risk of harmful residues. The levels that can be associated with clean or dirty are typically determined based on the exposed environment where the part will be deployed. What is acceptably clean for one segment of the industry may be unacceptable for more demanding segments. As circuit assemblies increase in density, understanding cleanliness data becomes more challenging. The risk of premature failure or improper function is typically site specific. The problem is that most do not know how to measure or define cleanliness nor can they recognize process problems related to residues. A new site specific method has been designed to run performance qualifications on boards built with specific soldering materials, reflow settings and cleaning methods. High impedance measurements are performed on break off coupons designed with components geometries used to build the assembly. The test method provides a gauge of potential contamination sources coming from the assembly process that can contribute to electrochemical migration.

KYZEN Corporation

Reactivity Of No-Clean Flux Residues Trapped Under Bottom Terminated Components

Technical Library | 2017-07-20 15:18:15.0

As electronic devices increase functionality in smaller form factors, there will be limitations, obstacles and challenges to overcome. Advances in component technology can create issues that may have time delayed effects. One such effect is device failure due to soldering residues trapped under bottom terminated components. If the residues trapped under the component termination are active and can be mobilized with moisture, there is the potential for ion mobilization causing current leakage.

Kester

Manufacturing Considerations When Implementing Voc-Free Flux Technology

Technical Library | 1999-05-07 11:44:26.0

In 1990 the United States Environmental Protection Agency Issued the Clean Air Act. The Clean Air Act and subsequent amendments are designed to limit the use of chemicals that contain volatile organic compounds (VOCs). The document goes into great detail setting limits for allowable VOC emissions for different industries.

Kester

The Nature of White Residue on Printed Circuit Assemblies

Technical Library | 1999-05-07 10:47:00.0

White residue remaining after cleaning circuit board assemblies can be caused by a variety of chemicals and reactions. Rosin and water-soluble fluxes, circuit board resins and epoxies, component materials and other contamination all contribute to this complex chemistry. This paper discusses many of the sources of the residues that seem to be an ever-increasing occurrence.

Kester

Electrochemical Methods to Measure the Corrosion Potential of Flux Residues

Technical Library | 2017-07-27 16:51:57.0

Reliability Expectations of Highly Dense Electronic Assemblies is commonly validated using Ion Chromatography and Surface Insulation Resistance. Surface Insulation Resistance tests resistance drops on both cleaned and non-cleaned circuit assemblies. It is well documented in the literature that SIR detects ionic residue and the potential of this residue to cause leakage currents in the presence of humidity and bias. Residues under leadless components are hard to inspect for and to ensure flux residue is totally removed. The question many assemblers consider is the risk of residues that may still be present under the body of components.

KYZEN Corporation

  1  

kester no clean searches for Companies, Equipment, Machines, Suppliers & Information

Void Free Reflow Soldering

World's Best Reflow Oven Customizable for Unique Applications
Circuit Board, PCB Assembly & electronics manufacturing service provider

High Precision Fluid Dispensers
PCB Handling with CE

High Throughput Reflow Oven
Encapsulation Dispensing, Dam and Fill, Glob Top, CSOB

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
PCB Depanelizers

"回流焊炉"