Technical Library | 2007-08-16 13:34:31.0
While experienced inspectors may be able to determine the aesthetic differences between a lead-free PCB assembly and a tin-lead version, one cannot rely on the "experienced eye". "Less wetting out to the pad edges" (Figure A) and "graininess and lack of shininess of the solder joint" (Figure B) are typical comments about some lead-free solder joints. However, in cases where a Nitrogen atmosphere was present during the reflow of the solder joint (Figure C), there will be little visual differences between the lead free alloys and their tin-lead counterparts.
Technical Library | 2009-06-11 19:27:21.0
The shock reliability of solder joints has become a major issue for the electronic industry partly because of the ever increasing popularity of portable electronics and partly due the transition to lead free solders.
Technical Library | 2010-02-10 23:50:23.0
The electronics industry has recently undertaken the transition to lead-free processing as a direct consequence of the RoHS directive, which came into force in July 2006. However, this is unlikely to be the last transition required since the European Solvent Emissions Directive, 1999 is starting to be implemented and enforced by national governments. This is resulting in pressure on larger manufacturers, currently emitting more than 5 tonnes of solvent vapour per annum to take steps to limit and reduce their emissions.
Technical Library | 2013-05-16 15:52:00.0
In response to a growing concern within the Electronic Industry to the transition to Halogen-Free laminates (HFR-Free) within the Client Market space (Desktop and Notebook computers) iNEMI initiated a HFR-Free Leadership Workgroup to evaluate the readiness of the Industry to make this transition. The HFR-Free Leadership WG concluded that the electronic industry is ready for the transition and that the key electrical and thermo-mechanical properties of the new HFR-Free laminates can meet the required criteria. The HFR-Free Leadership WG verified that the laminate suppliers can meet the capacity demands for these new HFR-Free laminates and developed a "Test Suite Methodology" (TSM) that can facilitate the comparison and choice of the right laminate to replace brominated FR4 in the Client space... First published in the 2012 IPC APEX EXPO technical conference proceedings.
Technical Library | 2014-01-02 15:56:55.0
With ROHS compliance the transition to lead-free is inevitable. Several lead-free alloys are available in the market and its reliability has been the main concern. The results from this experimental research aims at making a comparison of different lead-free alloy combinations. Thermal shock and drop tests are a part of this experimental study.
Technical Library | 1999-07-21 08:49:49.0
As the role of direct-chip-attachment increases in the electronics industry, the reliability and performance of COB packaging materials becomes an increasing concern. Although many factors influence component reliability, the biggest determinants of performance are often the glass transition temperature (Tg) and the coefficient of thermal expansion (CTE) of the encapsulant or underfill. This paper discusses exactly what these properties are, how they are measured, and why they are important to device-reliability.
Technical Library | 2007-05-30 19:30:22.0
Transition to lead-free is accelerating and when considering constraints related to lead-free and conventional solder pastes, one concern is rising: flexibility. It would be dangerous to commit to lead-free only while the technology is not yet stabilized. Manufacturers need to consider all of the issues related to lead-free and need to find flexible equipment which are able to adapt to both conventional and lead-free constraints.
Technical Library | 2014-06-26 16:43:12.0
Edgebond adhesives have been widely used by the industry for improving the shock performance of area array packages. Most of the studies focus on the impact of material properties, such as coefficient of thermal expansion (CTE) and glass transition temperature (Tg), on reliability at room temperature. However, the operating temperature of a component on the printed circuit board bonded with edgebond adhesive can be close to or exceed Tg of the adhesive, where the material properties may be very different than at room temperature.
Technical Library | 2021-08-11 01:00:37.0
Conformal coatings and potting materials continue to create issues for the electronics industry. This webinar will dig deeper into the failure modes of these materials, specifically issues with Coefficient of Thermal Expansion (CTE), delamination, cracking, de-wetting, pinholes/bubbles and orange peel issues with conformal coatings and what mitigation techniques are available. Similarly, this webinar will look at the failure modes of potting materials, (e.g Glass Transition Temperature (Tg), PCB warpage, the effects of improper curing and potential methods for correcting these situations.
Technical Library | 2008-04-29 15:50:45.0
The electronics industry is undergoing a materials evolution due to the pending Restriction of Hazardous Substances (RoHS) European Directive. Printed wiring board laminate suppliers, component fabricators, and printed wiring assembly operations are engaged in a multitude of investigations to determine what leadfree (Pbfree) material choices best fit their needs. The size and complexity of Pbfree implementation insures a transition period in which Pbfree and tin/lead solder finishes will be present on printed wiring assemblies