Water soluble lead-free solder paste is widely used in today’s SMT processes, but the industry is slowly moving away from water soluble solder pastes in favor of no-clean solder pastes. This shift in usage of solder paste is driven by an effort to eliminate the water wash process. Some components cannot tolerate water wash and elimination of water washing streamlines the SMT process. Despite this shift, certain applications lend themselves to the use of water soluble solder paste.This paper details the research and development of a new water soluble lead-free solder paste which improves on the performance characteristics of existing technologies.

FCT ASSEMBLY, INC.

The Nature of White Residue on Printed Circuit Assemblies

Technical Library | 1999-05-07 10:47:00.0

White residue remaining after cleaning circuit board assemblies can be caused by a variety of chemicals and reactions. Rosin and water-soluble fluxes, circuit board resins and epoxies, component materials and other contamination all contribute to this complex chemistry. This paper discusses many of the sources of the residues that seem to be an ever-increasing occurrence.

Kester

Impact of Dust on Printed Circuit Assembly Reliability

Technical Library | 2013-05-09 14:35:18.0

Atmospheric dust consists of solids suspended in air. Dust is well known for its complex nature. It normally includes inorganic mineral materials, water soluble salts, organic materials, and a small amount of water. The impact of dust on the reliability of printed circuit board assemblies (PCBAs) is ever-growing, driven by the miniaturization of technology and the increasing un-controlled operating conditions with more dust exposure in telecom and information industries... First published in the 2012 IPC APEX EXPO technical conference proceedings.

CALCE Center for Advanced Life Cycle Engineering

Using Hansen Space to Optimize Solvent Based Cleaning Processes for Manufacturing Electronic Assemblies.

Technical Library | 2009-07-09 17:23:07.0

Sometimes you just cannot clean with water. Good examples of this are: circuits with batteries attached, cleaning prior to encapsulation, ionic cleanliness testing, and non-sealed or other water sensitive parts. High impedance or high voltage circuits need to be cleaned of flux residues and other soils to maximize performance and reliability and, in these types of circuits; water can be just as detrimental as fluxes. When solvent cleaning is called for, Hansen solubility parameters can help target the best solvent or solvent blend to remove the residue of interest, and prevent degradation of the assembly being manufactured. In short, using this approach can time, manufacturing cost and reduce product liability.

Austin American Technology

Reduced Oxide Soldering Activation (ROSA)

Technical Library | 2007-07-19 15:15:11.0

ROSA is a surface restoration technique that removes hard to reduce species like metal oxides or sulfides. At the time of its development, the focus was on solderability and compliance to environmental regulations. Industry trends and regulatory changes as a result of the Montreal Protocol were the driver for much of the concern over environmental compliance. The result was an increase in the development of no-clean and water soluble fluxes and the removal of halogenated cleaning chemistries.

Electronics Manufacturing Productivity Facility (EMPF)

Effect of BGA Reballing and its Influence on Ball Shear Strength

Technical Library | 2013-07-11 15:22:40.0

This research paper will focus on the effect of various parameters that are used to reball a BGA and their effect on the overall shear strength. Factors that will be looked at include the type of BGA (SAC305 or 63Sn/37Pb), the alloy used to reball (SAC405 or 63Sn/37Pb), the type of flux used (Water Soluble or No Clean), and the environment in which reballing takes place (Nitrogen or Ambient).

MARTIN (a Finetech company)

CHANGING THE RULES OF STENCIL DESIGN

Technical Library | 2023-05-22 16:42:56.0

Nano-coatings are applied to solder paste stencils with the intent of improving the solder paste printing process. Do they really make a noticeable improvement? The effect of Nano-coatings on solder paste print performance was investigated. Transfer efficiencies were studied across aperture sizes ranging from 0.30 to 0.80 area ratio. Also investigated were the effects of Nano-coatings on transfer efficiencies of tin-lead, lead-free, water soluble, no-clean, and type 3, 4, and 5 solder pastes. Solder paste print performance for each Nano-coating was summarized with respect to all of these variables.

FCT ASSEMBLY, INC.

Fill the Void II: An Investigation into Methods of Reducing Voiding

Technical Library | 2018-10-03 20:41:44.0

Voids in solder joints plague many electronics manufacturers. Do you have voids in your life? We have good news for you, there are many excellent ways to "Fill the Void." This paper is a continuation of previous work on voiding in which the following variables were studied: water soluble lead-free solder pastes, a variety of stencil designs, and reflow profiles. Quad Flat No-Lead (QFN) component thermal pads were used as the test vehicle. The voiding results were summarized and recommendations were made for reduction of voiding.

FCT ASSEMBLY, INC.

Size Matters - The Effects of Solder Powder Size on Solder Paste Performance

Technical Library | 2020-10-27 02:02:17.0

Solder powder size is a popular topic in the electronics industry due to the continuing trend of miniaturization of electronics. The question commonly asked is "when should we switch from Type 3 to a smaller solder powder?" Solder powder size is usually chosen based on the printing requirements for the solder paste. It is common practice to use IPC Type 4 or 5 solder powders for stencil designs that include area ratios below the recommended IPC limit of 0.66. The effects of solder powder size on printability of solder paste have been well documented. The size of the solder powder affects the performance of the solder paste in other ways. Shelf life, stencil life, reflow performance, voiding behavior, and reactivity / stability are all affected by solder powder size. Testing was conducted to measure each of these solder paste performance attributes for IPC Type 3, Type 4, Type 5 and Type 6 SAC305 solder powders in both water soluble and no clean solder pastes. The performance data for each size of solder powder in each solder paste flux was quantified and summarized. Guidance for choosing the optimal size of solder powder is given based on the results of this study.

FCT ASSEMBLY, INC.

  1  

water soluble solder[0] searches for Companies, Equipment, Machines, Suppliers & Information

PCB Handling with CE

Training online, at your facility, or at one of our worldwide training centers"
Voidless Reflow Soldering

High Resolution Fast Speed Industrial Cameras.
PCB Handling Machine with CE

High Precision Fluid Dispensers


SMT & PCB Equipment - MPM, DEK, Heller, Europlacer and more...