SMTnet Express, July 24, 2014, Subscribers: 22981, Members: Companies: 13953, Users: 36523 Copper Wire Bond Failure Mechanisms. Randy Schueller, Ph.D.; DfR Solutions Wire bonding a die to a package has traditionally been performed using either
Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure Pd-Layers SMTnet Express October 11, 2012, Subscribers: 25550, Members: Companies: 9005, Users: 33789 Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure
SMTnet Express, September 24, 2015, Subscribers: 23,507, Members: Companies: 14,658, Users: 39,014 Gold Stud Bump Flip Chip Bonding on Molded Interconnect Devices Dick Pang, Weifeng Liu, Anwar Mohammed, Elissa Mckay, Teresita Villavert and Murad
SMT Express, Volume 2, Issue No. 9 - from SMTnet.com Volume 2, Issue No. 9 Thursday, September 14, 2000 Featured Article Return to Front Page Book Review Reviewed by Dave Fish (davef ), Pandion Electronics, Inc Title: Wire Bonding
SMTnet Express, September 7, 2017, Subscribers: 30,782, Members: Companies: 10,712, Users: 23,761 Challenges on ENEPIG Finished PCBs: Gold Ball Bonding and Pad Metal Lift Young K. Song and Vanja Bukva; Teledyne DALSA As a surface finish for PCBs
Drop Impact Reliability of Edge-bonded Lead-free Chipscale Packages Drop Impact Reliability of Edge-bonded Lead-free Chipscale Packages This paper presents the drop test reliability results for edge-bonded 0.5mm pitch lead-free chip scale
Gold Wire Bonding Performance and Reliability of ENEPIG Surface Finishes Gold Wire Bonding Performance and Reliability of ENEPIG Surface Finishes The expression "multifunctional PCB", as a synonym for a PCB which is applicable with a variety