Electronics Forum | Tue Oct 05 10:13:48 EDT 1999 | Frank Fossett
I am a new employee at a company that has had a large turnover of employees over the past year. I am working on a board (components on one side only), the engineer wants to use an .035 pad with a .012 dia. hole, there are no via's under the zero clea
Electronics Forum | Tue Oct 05 02:47:01 EDT 1999 | Eric
| Hi everyone, I need some help on the whole process of double sided surface mount. We have been doing surface mount for about 3 months and we're getting ready to take on our first doule sided board. I just need some step by step process regarding so
Electronics Forum | Fri Oct 01 05:03:28 EDT 1999 | Wolfgang Busko
| | | I am having problems processing immersion gold boards. The achieved solder joints appear acceptable a la IPC-A-610, but the resultant joint does not fully cover the land, i.e. you can still see an outline of gold pad. | | | What is the best way
Electronics Forum | Mon Sep 27 17:18:57 EDT 1999 | Erik
What selective soldering products should I use for a low production rate, high-mix product line? I am looking to get rid of some hand soldering. I have seen exselect (selective soldering pot method), pillarhouse (small flow solder nozzle with robot),
Electronics Forum | Mon Sep 27 17:52:16 EDT 1999 | Scott Cook
| What selective soldering products should I use for a low production rate, high-mix product line? I am looking to get rid of some hand soldering. I have seen exselect (selective soldering pot method), pillarhouse (small flow solder nozzle with robot
Electronics Forum | Tue Sep 28 10:22:29 EDT 1999 | John Susicki
| What selective soldering products should I use for a low production rate, high-mix product line? I am looking to get rid of some hand soldering. I have seen exselect (selective soldering pot method), pillarhouse (small flow solder nozzle with robot
Electronics Forum | Fri Oct 01 09:45:53 EDT 1999 | Andrew W. Dalrymple
| We are looking for a midwest board design house - Mike Weekes - 630 595 2300 x292 or email me at mweekes@phoenixofchicago.com | | I am starting up a PWB Design Service Company. We are Currently in Dallas. My partner and I have 25 years experia
Electronics Forum | Thu Sep 23 09:28:49 EDT 1999 | Earl Moon
| | Hiya, | | | | Could anyone please suggest recommended manufacturers of | | IR rework stations for the removal of various SMT comps. | | | | Cheers | | | Why IR ? Ok, I�ve seen only one but that thing burnt the PCB before the solder was meltin
Electronics Forum | Thu Sep 23 15:32:32 EDT 1999 | Earl Moon
| | Hiya, | | | | Could anyone please suggest recommended manufacturers of | | IR rework stations for the removal of various SMT comps. | | | | Cheers | | | I have 2 customers who went from hot air system to a PDR and they love it. The system wil
Electronics Forum | Tue Sep 21 13:10:10 EDT 1999 | Dave F
| Dear All, | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | I mean that I wonder why we use