Electronics Forum | Thu May 04 17:14:11 EDT 2000 | Boca
Solder 'follows' heat, sounds like the fab is heating up faster than the component. Or the components are solderability 'chanllenged' and the paste turns liquid, and would rather spead out on the land than wet to the component termination. Are thes
Electronics Forum | Wed May 03 16:33:27 EDT 2000 | Mark
Panasert tech support is 800 308 0891. It is 24 /7 and offers pretty good service. On the MV100 I'd ask for Pete Turner.
Electronics Forum | Tue May 02 19:29:03 EDT 2000 | Peter van den Berg
We're looking for a source of SMT links (Jumpers) 8mm - 10mm(.312in -.4in)long, capable of being placed by Panasonic MV2 series or MPA machines. Does anyone manufacture a feeder that creates links on demand?
Electronics Forum | Mon May 08 16:56:00 EDT 2000 | Peter van den Berg
Thanks Dave, we already use zero ohm resistors. What we're looking for is a flexible (bendable) jumper.
Electronics Forum | Fri May 05 14:32:14 EDT 2000 | C.K.
I read my posting again, and it didn't sound right....what I meant was slow down your conveyor speed BY .5 to 1 FPM. So, if you're running @ 4 FPM, slow it down to 3.0 to 3.5 FPM.
Electronics Forum | Tue May 02 11:21:43 EDT 2000 | �ngelo Marques
We have some Quad (QSA-30) machines, and i get better results when i optimize a program manually of the one that when i utilize the optimizer of the machine. Somebody knows a better software, than i stop using a manually optimizer. Sory me English. �
Electronics Forum | Tue May 02 11:50:26 EDT 2000 | Dan Foose
The first step in pinpointing the exact source of the fibers is to have them identified. Are they fiber glass, epoxy or flux? Or are they something else? I can help you with this if you want. Check out mfg-answers.com\ .
Electronics Forum | Fri May 05 14:44:35 EDT 2000 | Kal Chakraborty.
Hi Ashok, Is there any rework process on those assembl./PWB ..if yes --what kind of tools are your operators using now ...brush? spudger? cloths (is it lint free?) ect. I hope you are not talking about nodules in the hole barrel. Regards Kc.
Electronics Forum | Sat May 06 08:12:21 EDT 2000 | Dave F
Joe: That's what we do ... when the trend line is downward and below 40�C we start thinking. Apparantly, that's exactly what you do, except it's a matter of degree. Good luck. Dave F
Electronics Forum | Mon May 01 15:04:15 EDT 2000 | Ernie Miller
I need a good cleaning cycle for leaded brass (CuZn39Pb3). Product to be ni/au loose peice plated