Electronics Forum | Fri May 29 16:07:55 EDT 1998 | Steve Gregory
| | Thanks Steve- | Here is the whole story: | | The solder balls are appearing all over, similar to a | splatter. They are relatively small. We are using H-Technologies | S-HQ no-clean solder paste. The stencil is 6 mil and the boards | are ru
Electronics Forum | Fri Apr 10 20:35:59 EDT 1998 | Steve Gregory
| | We are having a bridging problem with SOIC 14,16 and 20 pin devices during flow solder of the bottom side of our boards. This bridging occurs about half way up the lead between the board and the body of the IC. The chip parts are no problem. T
Electronics Forum | Mon Apr 13 08:42:32 EDT 1998 | Bob Silveri
| | | | We are having a bridging problem with SOIC 14,16 and 20 pin devices during flow solder of the bottom side of our boards. This bridging occurs about half way up the lead between the board and the body of the IC. The chip parts are no proble
Electronics Forum | Thu Mar 05 13:17:19 EST 1998 | Justin Medernach
| Hello everyone! | Does any know anything about bare board size variations? | Is there a spec. or tolerance? | I'm running small lots of boards and during the screen printing process | I find that I cannot paste each board perfectly.I've tried other
Electronics Forum | Fri Jan 11 17:14:13 EST 2002 | davef
We have one product with electroless nickel, immersion silver solderability protection. We do not purport to be experts, but like many things, have seemingly boundless opinions. Side note: There are a least three different [maybe five] imm silver
Electronics Forum | Thu Jul 10 09:55:47 EDT 2003 | davef
A reading of the pictures is: A1: Looks like pad [B1] is smaller than the other pads. It�s weird that the pads are such different colors. A2: Looks like pad [B1] is smaller than the other pads. Solder mask opening [B1] is misregistered and seems s
Electronics Forum | Tue Jan 17 05:02:33 EST 2006 | grantp
Hi, I was replying to this thread appearing suddenly. However I have run both machines, and I paid for them myself because I run my own company, and so the choices I made, I personally had to pay for. Also, anyone who's been on this forum for a whi
Electronics Forum | Mon Aug 02 09:26:15 EDT 2004 | davef
Q1: How do you define torque setting for screw? A1: Talk to people at your nut supplier. Some nut suppliers post torque tables on the web. For instance: http://www.thelenchannel.com/1torque.html http://www.marfas.com/Ttorque.shtml http://www.pac
Electronics Forum | Tue Apr 23 15:36:27 EDT 2019 | davef
Josh, are you setting someone up with these questions? Answers to your questions related to the subject line follow: Q1. Does the Epoxy Solder Mask Layer of a PCB protect against moisture absorption? Is this a primary function of the solder mask?
Electronics Forum | Fri Mar 17 07:51:49 EST 2000 | Peter Barton
John, I have had previous experience of immersion silver coated PCB's in place of HASL coated type using no-clean processing with little or no problem at all. All of the process parameters were left unchanged. There is a very minor difference in th