Electronics Forum | Tue Jun 13 23:16:32 EDT 2006 | mrduckmann2000
WE LOOKED INTO THE YESTECH AND THE MIRTECH. TODAY WE ARE INSTALLING OUR NEW MIRTECH AOI MACHINE. WE CHOSE THIS MACHINE OVER THE YESTECH BECAUSE OF IT'S OFFERINGS. THE YESTECH WAS A CLOSE SECOND. I WILL POST LATER ON THE PROGRAMMING, THEY ARE ALL
Electronics Forum | Mon Jun 26 10:45:59 EDT 2006 | AOI Tech
Yestech,Yestech,Yestech Best friend to those of us in the US!!!!!!!That's all I'm going to say
Electronics Forum | Thu May 25 11:50:49 EDT 2006 | patrickbruneel
ERA presentation to the EU Commission On RoHS exempt category 8 and 9 http://ec.europa.eu/environment/waste/pdf/era_presentation.pdf I will not further comment because all I can do is shake my head (for now) Patrick
Electronics Forum | Fri May 26 11:06:30 EDT 2006 | pjc
Thanks for posting this Patrick. My head has finally stopped spinning after reading that document. Unbelievable is all I can say.
Electronics Forum | Fri May 26 11:54:21 EDT 2006 | SMT User
Would any of you be willing to interpet this a little? I believe I get the gist of it, but woulf like more info.
Electronics Forum | Thu May 25 15:14:07 EDT 2006 | H
Anyone think that this, http://img336.imageshack.us/my.php?image=nodule27wc.jpg, is a nodule which will eventually grow into a tin whisker? Observe the plating on the component lead. Thanks in advanced for opinions.
Electronics Forum | Thu May 25 15:31:08 EDT 2006 | samir
H, I tried without the commaat the end http://img336.imageshack.us/my.php?image=nodule27wc.jpg Seems to work. IMO, it looks like questionable component plating and not this so-called "nodule".
Electronics Forum | Thu May 25 16:50:34 EDT 2006 | patrickbruneel
This sure doesn't look very healthy. The important things to know are A) You see this already right after reflow B) Is this showing up after the board has been in use for a while If you could answer these questions we could take it a step further. P
Electronics Forum | Fri May 26 11:44:36 EDT 2006 | H
Patrick: The image that you see was from a unit that was known to have gone through a 5-year environmental life test. However, we took another board, pre-refow, and scoped a similar device. It exhibited the same grainy component plating.
Electronics Forum | Fri May 26 10:04:06 EDT 2006 | jdengler
Paul, The paste you use is another variable. As Pete recommends to know the real answer you need a DoE. Jerry